    Ok... I just traded my bottle of Argon for another one.... it's a 300cf
    My first bottle was charged to 1600psi and it was fall so a little warmer
    This second bottle is charged to 2400psi and it was in my truck out in 30 degree weather all night.

    Did I get ripped off on the first bottle?
    What do they normally fill these to?
    Last edited by CGCINC; 02-10-2012 at 03:37 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    Also, I think I have a lifetime lease through this company (Airgas)
    I'm wanting to get my bottles through another company that is closer to me. Can I just turn in my bottle when its empty and thats, that, or do they charge you to leave like the phone companys do.....?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by CGCINC View Post
    Also, I think I have a lifetime lease through this company (Airgas)
    I'm wanting to get my bottles through another company that is closer to me. Can I just turn in my bottle when its empty and thats, that, or do they charge you to leave like the phone companys do.....?
    Probably depends on the fine print in your paperwork, I don't see how they could charge you any more when you already have a lifetime lease. Switching to the other company without additional cost may depend on whether you got an unmarked cylinder(no problem at all, just like trading in an empty keg) or how fast and loose the LWSes in your area play with each others bottles.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  4. #4

    Default

    It never get one above 2000 psi. I am getting ripped, but the price is good so I guess it equals out.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  5. #5

    Default

    Quote Originally Posted by CGCINC View Post
    Also, I think I have a lifetime lease through this company (Airgas)
    I'm wanting to get my bottles through another company that is closer to me. Can I just turn in my bottle when its empty and thats, that, or do they charge you to leave like the phone companys do.....?
    They no longer do lifetime leases, you now have to pay every year to lease. I would not turn that bottle in, but I would get one from another company. Sometimes you can get a bottle from Airgas with out their name, and if you get one find a gas pony location at a Northern Tool or Tractor Supply and trade it in! Gas Pony's are owner bottles and they will make you pay 25-30$ to swap to gas pony plus the gas. You walk away with an owner bottle without any company name, and you can fill your new bottle anywhere.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  6. #6

    Default

    My local airgas only sells up to 80 cf tanks Ar, C25, when you buy the tank they tell you the first fill in it is free. I think they may give you one that they took back partially full.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  7. Default

    Yes, but probably not purposefully. The bottles are usually filled twice. Because of the size of the bottle the first full is called a Hot fill... The compression of gas inside the bottle makes the gas get hot and reads higher. The bottle is let cool, then topped off. They may have gotten busy and forgot to top it off.

  8. #8

    Default

    Quote Originally Posted by Gwaltnak View Post
    Yes, but probably not purposefully. The bottles are usually filled twice. Because of the size of the bottle the first full is called a Hot fill... The compression of gas inside the bottle makes the gas get hot and reads higher. The bottle is let cool, then topped off. They may have gotten busy and forgot to top it off.
    Well, that along with the poor service and bad attitudes I get there makes me think I'm taking my business elsewhere.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  9. #9
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Different types of compressed gas cylinders are rated for different pressures. For example, if the bottle has a star imprinted on it (or two), it indicates the cylinder can handle additional pressure.

    That said, my experience is that the local welding supply in my neck of the woods doesn't always give people what they bargain for. Still, they are the best option around. Just don't blindly trust the cubic feet printed on the invoice is correct.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  10. #10
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by jakeru View Post
    Just don't blindly trust the cubic feet printed on the invoice is correct.
    Do you usually carry a gage with you to check?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  11. #11

    Default

    AirGas is notorious for bad service. There must be *some* that do well... but i tend to avoid them on principle now, after having so many problems with them in the past.
    I just don't know how they stay in business. One time at an AirGas in North Carolina i gave them 3 empty bottles, and they tried to give me back 2 fulls and 1 empty in exchange. Charged me for 3, tho. Caught it before i left their dock.

    I usually crack the nozzle on the bottle real quick to check it before i take it home. After you've hooked up enough of them you know what the 'whoosh' of a full bottle sounds like in pitch and volume (and you should be cracking the valve open before you ever connect it to your regulator anyway, to clean out any dirt or dust that may have gotten in the fitting).
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  12. #12
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Quote Originally Posted by redbeard View Post
    Do you usually carry a gage with you to check?
    I usually don't, just because it's inconvenient for me to do every time, and also, if a cylinder they brought out for me is underfilled, but only by 15-20% (as they often are), it is not actionable information for me (I am not going to reject it if it's underfilled by 15-20%, I am still going to take it. They have no means at their location to "top off" a cylinder with additional pressure, what they have is what they have, unless you want to try swapping with another cylinder.)

    I think I only ran into a cylinder being underfilled less than that amount once... and they "made good" on it for me. A bit of a hassle to bring it back but they gave me a free fresh fill for it. They are real good to work with and have fair prices, (even considering their commonly underfilled cylinders.)
    '13 Everlast 255EXT
    '07 Everlast Super200P

  13. #13

    Default

    Quote Originally Posted by CGCINC View Post
    Ok... I just traded my bottle of Argon for another one.... it's a 300cf
    My first bottle was charged to 1600psi and it was fall so a little warmer
    This second bottle is charged to 2400psi and it was in my truck out in 30 degree weather all night.

    Did I get ripped off on the first bottle?
    What do they normally fill these to?
    They should have a gauge and read the pressure before they give it to you. The pressure when refilled should read above 2100 psi, sometimes up to 2500 depending on temperature.

    If your LWS does not read the pressure in front of you, then it is time to find another LWS. Mine does and they say it is company policy as an empty might find its way by mistake to the filled area.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  14. #14

    Default

    I finally exchanged my bottle today. I got it from the machine shop manager at work (was his personal bottle for previous home use, no use for it anymore). It is a 155cf bottle. I ran out the other night while working on my bike frame.

    LWS that I went to was Matheson Gas in Johnstown, PA. Used to be Valley National Gas. Total out the door was $36.48. Bottle was filled to about 2100 or so. Bottle I got is rated at 2084psi. Bottle I exchanged was last Hydro'd in '97. No issues at all with the exchange.

    This was the first time I had been to this store. Chatted with the desk clerk for a minute, then headed off to work. Didn't have any problems at all in dealing with them. No poor attitudes, nothing, just good customer service for a walk-in (me) buying $36 worth of gas.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  15. #15
    Join Date
    Dec 2011
    Location
    West Virginia
    Posts
    24

    Default Airgas

    Quote Originally Posted by CGCINC View Post
    Ok... I just traded my bottle of Argon for another one.... it's a 300cf
    My first bottle was charged to 1600psi and it was fall so a little warmer
    This second bottle is charged to 2400psi and it was in my truck out in 30 degree weather all night.

    Did I get ripped off on the first bottle?
    What do they normally fill these to?
    I've heard from many people and one guy that worked for airgas that they do rip people off all the time. Someone told my brother they actually take bottles people bring in and take them and act like the person didn't bring the bottle at all.

Similar Threads

  1. 100 PSI argon flo?????
    By stretch in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 32
    Last Post: 06-09-2016, 08:51 PM
  2. Argon / co2 question
    By DaveO in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 5
    Last Post: 06-10-2014, 02:20 PM
  3. Why 100% Argon or Argon/CO2 75/25%
    By mdennis in forum General Welding Questions
    Replies: 6
    Last Post: 08-09-2013, 04:11 AM
  4. Air/Argon
    By ChadP in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 02-09-2013, 09:20 PM
  5. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •