BillI have the HF bench top unit and use the same stuff had a bigger tip I think. Soda is the way to go will not harm glass and just wash off. FYI dont wash it off till you are ready to make ready to paint as it provides a protective coating that helps to reduce rust. You have to add Viniger to water to remove