My best friend runs a Nesmith Dirt Late Model. This is a GM crate motor series. He wanted to race really bad and borrowed an old set of headers. They were cracked pretty good and very rusty. This was a I just want to race tonight fix. These headers had been raced for 3 years by another friend, and needless to say we picked them out of the scrap pile. I did a little grinding, but not a major cleanup these headers were thin!
Power Arc 140st
27-32 amps
This is the first hole that I plugged
This was my first tig welds with my Power Arc 140st
![]()