7014 is the "sheet metal" rod and runs quite well on sheet metal. I've had good luck running 7014 3/32 on 12g sheet metal. Sometimes you may have to speed up a little keep from burning through your metal.
7014 is the "sheet metal" rod and runs quite well on sheet metal. I've had good luck running 7014 3/32 on 12g sheet metal. Sometimes you may have to speed up a little keep from burning through your metal.