Looks good I need to put a little more time into the graph paper before I start cutting. One thing I found is, I wish I would have given myself a little extra room for the shielding gas bottle in case I want to go to a larger bottle, also when I moved to K.C. the place i get my gas primarily stocks a slightly different size bottle than I was getting in CA. I used plumbers tape instead of chain the first time and cut it to exactly the right length for my first bottle so it would look nice and neat. now of course it's a bit short. leave yours long and adjustable to save yourself the double work. You might even want enough room for a second bottle, Jakearu loves his helium for tigging aluminum.