I am new to tig, and do not even have an Everlast yet...but looking. I have a Chiri UNT 3-in-1 unit. I would have asked on the WW forum, but expected I would get flamed for having a chinese unit. Everything works fine, except I have a question about initial startup.
I am using a WP-17 torch (no pedal), 1/16" 2% lanthanated sharp, Argon at 11cfh. Today welding 1/8" angle, with 1/16" 70S-6 filler, 65amps. This action has happened on other thicknesses of metal, and amp settings also.
When I first press the lever to initiate a weld, at once, the arc jumps and there is a POP. Like a small balloon being punctured. Then all settles down, and seems ok. Is this normal? It does not happen every time, random, as far as I can tell.
Not sure if it is argon, or only when I have too much distance from the work (long arc initially). The flowmeter could be incorrect, but I can get a good puddle and the weld looks fairly decent for a learner. So I think I have correct flow.
Any ideas I could check out further? I expect is probably operator induced if it is a problem.