TIG Lessons in N.C.?
Bought a PP205 and am brand new to welding. Researched online and watched all of Jody's videos. Definitely have gotten better, but now getting frustrated. Wanting to weld aluminum diamond plate .063. Been practicing on scrap.
Have cleaned with Acetone and dedicated stainless brush. Using Argon 7 lpm, 3/32 Lanth. Tung., 50 amps, 3/32 filler rod, 150 hz AC frequ, 30% AC Bal., etc...
Filler Rod continues to want to ball and absorbs on the Tungsten...feel like I spend more time grinding tungsten than under the hood.
Anyway, I am at the point to hire someone for lessons to get good habits and catapult the learning curve. I live in Charlotte...Does anyone have any recommendations or suggestions?