By using an oven, is the water content you're trying to get rid of in the rod or flux?
I was just wondering if I could just knock the flux off my 7018 and use it for TIG?..or do I still have to put it in the oven?
By using an oven, is the water content you're trying to get rid of in the rod or flux?
I was just wondering if I could just knock the flux off my 7018 and use it for TIG?..or do I still have to put it in the oven?