    I have now had my multi unit for just about a year. So far I have only used the tig and love it for that. I am new to stick but thought this project (home made boat float inflating 6 55gallon barrels for floatation ) would be a good one to try the stick on. Its an outside project as you can see at least for the tack up. The stick looks a bit messy as I am new to this. 1/8th wall tubing to 1/4 inch angle for most of it.

    At this time I have 3 questions.

    1. I am using 6013 rod, is this ok.

    2. Not sure to use electrode neg or pos....switched back and forth but did not seem to make much difference.

    3. If I want to go over all the welds by grinding and tig welding is that ok or is there contamination from the flux in the rod for me to tig weld. If I do try and tig it to clean things up I guess I should grind and brush?

  2. #2

    Default

    1) Yes, no problem. Just make sure you get good fusion and no slag in the middle of the joint.
    2) Unless specifically told to do otherwise, always electrode Postitive (reverse polarity)
    3) You should not tig over in this case. All you will do is overheat the tubing and make a large heat affected zone, making the area just outside of the weld weak and brittle.

    A 6013 will run well IF you clean the metal slightly with a grinder first.

  3. #3

    Default

    Thank you Mark...............I will grind and stick weld till its all good. Or good enough!........wayne

  4. #4
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    6013 is more of a temp repair low penetration rod for the reason it got nick named Farmer rod
    i would weld it up with some e6010/e6011 or some e7018
    Last edited by Wookie; 04-02-2011 at 06:35 AM.
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

Similar Threads

  1. Power I Mig 200 MIG STICK WELDER , how high should the amp gauge read on stick side
    By Tim L Rogers in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 01-22-2016, 04:42 AM
  2. Tig (ac/dc), mig, stick, plasma
    By scootarida1 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 11-27-2014, 01:25 AM
  3. The joy of DC stick
    By JohnT in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 08-25-2014, 01:56 AM
  4. some higher amp stick with PU 205
    By worntorn in forum Stick Welding (SMAW)
    Replies: 2
    Last Post: 05-07-2011, 12:18 PM
  5. Anybody use their 250 EX with the stick?
    By Nikola Tesla in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 03-28-2011, 01:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •