  1. #1

    Default Very first try with 200DX

    Well I got to do some welding today, These are my first bird turd passes
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMAG0299.jpg 
Views:	359 
Size:	148.1 KB 
ID:	4613   Click image for larger version. 

Name:	IMAG0300.jpg 
Views:	389 
Size:	146.7 KB 
ID:	4612  
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  2. #2

    Default

    When I first tried to make a pass I kept melting the crap out of the tungsten, I tried and tried to make adjustments and it still just globbed up and melted back the tungsten, I did this about 6 times grinding the tungsten back to a point. I kept looking online and at the owners manual until I realized that I had the torch plugged into the + and the ground clamp plugged into the -. Switched it around and Bingo works fine now.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  3. Default

    Hey, those aren't so bad. Better than what my very first tries looked like.

    You should now be at that hell-bent addicted stage (if you are like me anyway), where you could just burn hours and hours putting metal on metal.

    Keep at it!

  4. #4

    Default

    Yeah, I was up till 2 am last night lol
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  5. #5
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    My first words are Good Job! For a first try, looks pretty good. The only thing that will improve your skill is SEAT TIME!!. I would suggest that you get some 1/8" pieces of aluminum, in the 8"-10" x 3"-6" range, like at least a half dozen such pieces, and get practicing on aluminum. Your skill level (at least as far as my experience was) is that once you get real comfortable running aluminum, Steel and stainless are a snap!. Keep it up. By the way, have you noticed that once the helmet is down, and the arc is struck, everything else in the world disappears? It's extremely theraputic.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  6. #6

    Default

    Those look way better than my attempts so far.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  7. #7

    Default

    Thanx for the kind words and encouragement, I haven't tried AC with aluminum yet, I did go to the steel yard and grabbed a bunch of small strips/pieces of both mild steel and aluminum.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  8. Default

    Hi Buzz, congrats on the 200DX. I've had mine a little over a month and it's been a great machine for me. I'm betting that you're going to really like the way it handles aluminum once you get it set to your liking. The best advice I got when I was taking classes at my local community college was not to be afraid to put the pedal to it to get the puddle going since anything thicker than sheet really soaks up the heat.

    Gary

  9. #9

    Default

    Im getting a little better, I want to finish my welding cart project before I take on the Aluminum
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMAG0310.jpg 
Views:	358 
Size:	145.8 KB 
ID:	4628  
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  10. #10
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    See? just a little more practice, and your weld quality is waaay better! Keep up the great progress!
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  11. #11

    Default

    I am having a blast playing with this thing. It is so smooth, Like you said its therapeutic.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  12. #12

    Default

    Looks like your getting much better penetration. A little more practice moving straight and even and your golden. Looks good
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  13. #13

    Default

    WooHoo...
    another tig welder is born.

    With practice and time your hand will get steadier, your heat control easier to manipulate, your penetration complete and your weld spacing more and more even.
    It's all just practice, patience, and time.
    When i want to stretch my skills, i find harder and harder materials to master welding. Once you get the hang of using the pedal to control your puddle and getting complete penetration and get some good timing, i would get some aluminum scraps. hooda is right, it will force you to become a much better welder in order to get it to work, and your steel welds will become an order of magnitude better... but don't jump into it too early, you need to get an understanding of puddle and heat control, otherwise you're going to end up melting out a LOT of holes in metal in frustration. =)
    I weld thinner and thinner gauges of aluminum as i get better, and new metals that are harder and harder to weld- Like copper, brass, & titanium.

    Keep up the practice and you'll get it before long!
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  14. #14

    Default

    Im almost done with my welding cart, soon I'll start playing with AC and aluminum.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  15. Default

    I like to see posts showing the 200DX . In case anyone is interested this is actually one of my favourite models. It is actually only recently that you are starting to hear more from users with this welder
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  16. #16

    Default

    Looking very nice Buzz.
    What part of Minnesota are you from?
    Consistency is a good thing....unless you're consistently an idiot.

    Miller Matic 185
    Thermal Dynamics Pak Master 38xl
    Everlast 250EX

  17. #17

    Default

    Quote Originally Posted by Titan winch View Post
    I like to see posts showing the 200DX . In case anyone is interested this is actually one of my favourite models. It is actually only recently that you are starting to hear more from users with this welder
    Mine works great, I love this machine so far . I still have yet to try AC aluminum

    Quote Originally Posted by brad3579 View Post
    Looking very nice Buzz.
    What part of Minnesota are you from?
    Im in Minneapolis, you?
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  18. #18

    Default

    Quote Originally Posted by Buzz View Post
    Im in Minneapolis, you?
    Lino Lakes, just down the road
    Consistency is a good thing....unless you're consistently an idiot.

    Miller Matic 185
    Thermal Dynamics Pak Master 38xl
    Everlast 250EX

  19. #19

    Default

    Quote Originally Posted by brad3579 View Post
    Lino Lakes, just down the road
    Cool, Im trying to make out the car in your avatar, Camaro?
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

Similar Threads

  1. Buy the Powertig 200dx or save for The Dynasty 200dx
    By AfroPaul in forum TIG Welding (GTAW/GTAW-P)
    Replies: 40
    Last Post: 05-13-2013, 07:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •