    just got off the phone with my metal supplier and ordered some 1"x1"x1/4" aluminum angle. it may not be the best choice, but it will give me a chance to play with my 250ex. im not going to go to fancy, some casters, handle and a shelf. i will probably intergrate the water cooler into the frame, and have a spot for the bottle. havent drawn it up yet, but im thinking around 3' should be good. i was hoping to get it done this weekend, but the angle wont be ready till monday. so pics and specs will be up next week.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  2. #2
    Join Date
    Dec 2011
    Location
    RUSSIA.Sankt Peterburg
    Posts
    218

    Default

    With great interest will be watching for your project.
    I am also working on my welding cart .
    good luck.
    Ruslan
    EVERLAST Power Tig 255 EXT
    EVERLAST PP256
    PC300
    EWM Pico 162
    MERKLE mobimig 180K
    SELCO Genesis 352 pme

  3. #3

    Default

    I will be watching also. one inch aluminum sounds a little light. I am in process of building a cart also but it is 1 1/2x1/8 square tube. I will be adding pics and specs soon, but let me tell all I am not a fabricator or a welder so I am a little sheepish about throwing it on forum because of quality of everybody else project mine looks pretty crude. I will get some pics and post in a day or two.
    Bill

  4. #4

    Default

    Quote Originally Posted by 67cudafb View Post
    I will be watching also. one inch aluminum sounds a little light. I am in process of building a cart also but it is 1 1/2x1/8 square tube. I will be adding pics and specs soon, but let me tell all I am not a fabricator or a welder so I am a little sheepish about throwing it on forum because of quality of everybody else project mine looks pretty crude. I will get some pics and post in a day or two.
    Cuda, I put up a crappy project that I doubted was worthy and got a few pats on the back so don't worry about that, Everyone here is great, they follow moms rule, "If you don't have anything nice to say don't say anything at all."
    Miller Challenger 172 Mig
    Soon to be winner of a Powertig 210 EXT

    Wade Mortenson

  5. #5

    Default

    I'm always more interested in the designs and ideas than how pretty the welds are. My welding cart is an old supermarket shelf-stocker's cart. I'll post pics when I put a raised shelf on it to get the machines up around eye level, and magically produce a couple more feet of storage space.
    Last edited by Jake98; 01-14-2012 at 03:48 PM.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  6. #6

    Default

    I dont see why that stock would be too light.. If its built right, I bet it will be more than sturdy enough as a cart.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  7. #7

    Default

    Well got my aluminum today, turns out its only 1/8". To bad i started cutting it already. Basic specs are 2'L x20"W x3'H. Its only 2'9" in the back to have a slight angle. Ill have two pieces down the center on the top to support the plasma and tig. The middle will have a shelf to hold project 1, the water cooler. Ill put some abs tubing on the side to hold rod, and also have a small platform to hold the gas. The first pic is the highly accurate blueprint, and then just some cuts. I didnt get all the pieces cut tonight, maybe tommorrow.
    EDIT : did this on iphone, cant flip the pic sorry. Maybe if i find time tommorrow ill fix it.



    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  8. #8

    Default

    So i went in today, started tacking up the cart. Took a little bit to even get the settings down for ac. Ran into a few issues. One is since its aluminum, the heat distortion is greater and now its crooked. I still have to put the top on so maybe i can pull it back. Also welding inside corners is tough as i cant get in there. Finally my bud brought up a good point in since the thing is so light, the tig and plasma are going to make it very top heavy. I might end up putting the plasma on the middle shelf to help weight. But as for the actual material not being sturdy enough, with just the few tacks i have on now its plenty strong, stable and ridgid. Heres two pics of the shape. And yes thats an old 300.


    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  9. #9

    Default

    Got some work done tonight, decided to put the plasma on the middle to help weight. I was just using it to check fit and clearences.
    So the back pic shows that the cord and air hose just clear. Same with the front. I set the front back a few inches so that the connections at the front are protected and wont stick out past the cart. I cut the angles down so the fit flush. Everything is still basically tacked in place, once i have everything wherr im happy ill goto town welding.






    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  10. #10

    Default

    Click image for larger version. 

Name:	1edde3b2.jpg 
Views:	880 
Size:	115.7 KB 
ID:	4676


    Hey jerky - I flipped your drawing the right way.
    Some of the crap I use to keep busy:

    Everlast 200DX
    Millermatic 211 Mig
    Hypertherm Powermax 30 plasma cutter
    Lincoln Weld-Pak 100
    Century Stick welder
    Oxy set-up with Henrob 2000 torch
    Logan 200 lathe (60 years old)
    Jet band saw
    About 6 Harbor Freight grinders with different discs/wheels/brushes

  11. #11

    Default

    Looks good so far.. Are you going to add on to it to hold a bottle or two for the welder(s) that will sit on it?
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  12. #12

    Default

    It looks top heavy to me. Is that bottom shelf area to put a few cinderblocks on to help prevent tipping?
    Some of the crap I use to keep busy:

    Everlast 200DX
    Millermatic 211 Mig
    Hypertherm Powermax 30 plasma cutter
    Lincoln Weld-Pak 100
    Century Stick welder
    Oxy set-up with Henrob 2000 torch
    Logan 200 lathe (60 years old)
    Jet band saw
    About 6 Harbor Freight grinders with different discs/wheels/brushes

  13. #13

    Default

    My very old bed-rail welding cart has three shelves.

    TIG on top, MIG in the middle and PP60 on the bottom. So drop a plasma cutter on the bottom to prevent tipping.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  14. #14

    Default Heavy

    I stand corrected about strong enough. I have found out the hard way that I have over built my cart with 1.5x1.5x1/8 steel tube it is very heavy. Like I said I am not a fabracator and should have had better plan instead of winging it. I hope my next build will be better. Your cart looks great.
    Bill

  15. #15

    Default

    Well, dont ever use aluminium. My middle shelf wasent big enough for the plasma, so i took the handle off and jammed it it in there. I dont have casters yet so its probably going to wtay inthe corner for awhile.

    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  16. #16

    Default

    Looks good to me, why not use aluminum? I think it looks great and it would be great practice. I was curious too what you were going to do to move your bottles around? but maybe mobility wasn't important to you, that explains why casters weren't high on your shopping list...
    Miller Challenger 172 Mig
    Soon to be winner of a Powertig 210 EXT

    Wade Mortenson

  17. #17

    Default

    Can you show a close up of the welds, and tell us what settings you used? I am trying to get it right with aluminum now, and I am using the same thickness pieces as your stock.
    Some of the crap I use to keep busy:

    Everlast 200DX
    Millermatic 211 Mig
    Hypertherm Powermax 30 plasma cutter
    Lincoln Weld-Pak 100
    Century Stick welder
    Oxy set-up with Henrob 2000 torch
    Logan 200 lathe (60 years old)
    Jet band saw
    About 6 Harbor Freight grinders with different discs/wheels/brushes

  18. #18

    Default

    Most of the welds arnt that good because of going into an inside corner. But settings are as.... Main amps were at 125, pre flow at 2 seconds, post flow at 5 seconds, up slope is 2 seconds, down slope is 3 seconds, start and end amps at 50. I will have a place for the bottle at the back, but ya, not really concerned yet because my table is right there. Getting casters soon. I say dont use aluminum because of all the stress and distortion. My rack is crooked and bad. Ha ha ha. Also i was using 2% throiated tungsten as well with #6 cup
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

Similar Threads

  1. School project from Jerky (3g tig root)
    By jerky in forum Hobyist Projects
    Replies: 7
    Last Post: 02-20-2012, 04:23 PM
  2. Project #3 Another another Welding Cart
    By Buzz in forum Hobyist Projects
    Replies: 30
    Last Post: 02-17-2012, 06:22 AM
  3. PROJECT 3 from Jerky: coffin gas tank
    By jerky in forum Other Custom Fabrications
    Replies: 6
    Last Post: 01-30-2012, 05:41 PM
  4. PROJECT 1 from JERKY: tig cooler
    By jerky in forum Other Custom Fabrications
    Replies: 11
    Last Post: 12-30-2011, 10:50 PM
  5. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •