    I will check it out when I get to work tomorrow. I was just so frustrated that I just lef it alone, thinking it may be something simple I may have overlooked. Will post in the morning once I have a look at this area again. I am sure that I had a look over the entire board, thinking that it may be a pinched wire (to ground) but could not see anything. The problem was present even with the cover off though..


    Quote Originally Posted by srp View Post
    Hang in there Boosted, after you get it fixed you will love it. Make sure its not in stick mode, after you get the high frequency working, turn the start amps to about 25 amps, that really helps to get a clean and positive start.
    Yeah, I know that when it does work, it works great. I have a 4 year old 200dx in my shop and lover it. I have not had a single issue with it, and it has never let me down. The 250EX has a few times, and I hope once this is resolved that it is smooth sailing.
    Last edited by Boosted P; 03-06-2012 at 05:02 AM.

  2. #2

    Default

    Yea, you probably cut through one of the HF board wires when you put the cover back on. They lap over the side of the board (left side looking from the front). The board is mounted upside down, mid center towards the front of the machine on the left side.

    I can assure you the 250EX is the cream of our analog TIG units, you're just have a run of bad luck.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. Default

    Quote Originally Posted by everlastsupport View Post
    Yea, you probably cut through one of the HF board wires when you put the cover back on. They lap over the side of the board (left side looking from the front). The board is mounted upside down, mid center towards the front of the machine on the left side.

    I can assure you the 250EX is the cream of our analog TIG units, you're just have a run of bad luck.

    After messing around with it for a bit longer I found the issue.

    For some reason the "Pre Flow" knob was turned to about 5 seconds causing the start delay of the HF circuit. I never thought to look at that, and did not think to relate it to the actual "weld start" condition. It makes sense when you think about it, I just though of it as gas related only, and since I had gas flow did not think to mess with it.

    Thanks for all the suport, really appreciate it.

    Hope this is the last of any problems with this machine.

    Also, has Everlast though about a filter kit for the cooling fan? I have been using compressed air to keep the inside clean (blowing it all out with the cover off), but a filter system would be much better.
    Last edited by Boosted P; 03-06-2012 at 04:39 PM.

  4. Default

    Quote Originally Posted by Boosted P View Post

    Also, has Everlast though about a filter kit for the cooling fan? I have been using compressed air to keep the inside clean (blowing it all out with the cover off), but a filter system would be much better.
    Interesting point on this. The company I work for, we have cooling fans on some of the stuff we make/sell. It actually turned out to be more of a liability to have filters than to not have them.

    Without them, things get dirty and not so pretty. But WITH filters, customers would forget about them and neglect them (especially mounted in a rack). They would get plugged and cut off air until stuff starting overheating.

    Temperature causes exponentially increasing aging on electronic components, and it actually caused MORE failures than no filters at all.
    Vice Grips
    WD-40
    Duct Tape

  5. #5
    Join Date
    Dec 2011
    Location
    Knoxville, Tennessee
    Posts
    93

    Default

    Quote Originally Posted by Boosted P View Post
    After messing around with it for a bit longer I found the issue.

    For some reason the "Pre Flow" knob was turned to about 5 seconds causing the start delay of the HF circuit. I never thought to look at that, and did not think to relate it to the actual "weld start" condition. It makes sense when you think about it, I just though of it as gas related only, and since I had gas flow did not think to mess with it.

    Thanks for all the suport, really appreciate it.

    Hope this is the last of any problems with this machine.

    Also, has Everlast though about a filter kit for the cooling fan? I have been using compressed air to keep the inside clean (blowing it all out with the cover off), but a filter system would be much better.
    Just be careful to NOT get the nozzle too close to the boards when doing this. Sometimes the things attached to the boards aren't all that solid and compressed air can cause them to break loose.. Seen it happen before and it's almost impossible to figure out what all is damaged when that happens.. I use compressed air as well but I stay way back from the boards when doing that..

  6. Default

    We use compressed air in a can for computers because will do not want to spray air compressor oil all over our electrical components and that too, not to blow chips out of the board. LOL

Similar Threads

  1. PowerTig 250EX questions ---- foot pedal
    By 11Bravo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 09-07-2018, 03:53 AM
  2. 250ex replacement foot pedal
    By srhprerunner in forum TIG Welding (GTAW/GTAW-P)
    Replies: 15
    Last Post: 09-13-2012, 09:09 PM
  3. Micro 185 foot pedal problems.
    By airsickness in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 01-28-2012, 08:37 PM
  4. PowerTig 185 and 250EX foot pedal
    By TD2593 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-14-2012, 12:50 AM
  5. Foot Pedal and Torch on 250EX
    By Rugar in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 08-01-2010, 06:13 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •