your getting there! more you do , better you get. and it looks like your improving alot over your projects... keep up the work!
your getting there! more you do , better you get. and it looks like your improving alot over your projects... keep up the work!
Aluminum is a hard way to start but you picked up pretty fast.
Like said, you can see the improvements from the 1st to 2nd project. I know you have not had the unit long, I am impressed.
Keep the projects coming.
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
MD,
Nice job, that aluminum can be tough, you see that first "wiggle" and it's too late!!
Goat
When our welder was teaching me to TIG aluminum, he would have me tack together a three sided box, (two sides and a bottom) and then have me weld into the corner to drive the heat that way. This would teach me to watch for the "wiggle" and lay off before everything blew out. This was great way to practice for a novice.
On a side note, I watched this guy TIG two gum wrappers together, he had talent!!.