    Took me a few days to get to it, and a second try at getting it running, but the IMIG 200 is in place, working, and I am stoked. I think I originally had a grounding problem, but overcame that and ran the MIG first. With no calculator handy I was guessing at settings but still managed to get a passable looking weld- the first bead I ran was too tall, I know, but I played with it and it flattened out. Next time I'll have a calculator handy.

    Then I switched over to stick and burned a 6011 rod- I was amazed at the difference between this machine and my old Miller crackerbox. A completely different sound and the only way I can describe it is a smoother arc. I like the way a stick electrode smells during welding.

    So I am a very satisfied customer this evening, and have a project in mind to get some actual use out of the machine!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  2. #2

    Default

    I know those older transformer machines run like a beast, but I prefer inverter style welders for the smoother welding capabilities.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3

    Default

    I've used an I-MIG 200 for stick,.. If you think that the arc welding is great with your I-MIG 200, you should try a PowerArc 200. It is even more fun! We just got our I-MIG a couple days ago and it's great. We need some help dialing in settings. The wire is kinda lurchy, I believe it maybe us not knowing good settings.. We are running fluxcore. We tried different tensions on the drive rollers.

    Thanks for any help,
    ILP
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  4. #4

    Default

    Quote Originally Posted by I_Love_Plasma View Post
    I've used an I-MIG 200 for stick,.. If you think that the arc welding is great with your I-MIG 200, you should try a PowerArc 200. It is even more fun! We just got our I-MIG a couple days ago and it's great. We need some help dialing in settings. The wire is kinda lurchy, I believe it maybe us not knowing good settings.. We are running fluxcore. We tried different tensions on the drive rollers.

    Thanks for any help,
    ILP
    Open the cover, turn it on, pull the trigger and see what's happening. If the wire pushes the gun back while welding you either have a poor ground, not enough volts set or too much wire speed. I run an oversize tip with flux core (.045 with .035 wire) because the wire can be dirty or not perfectly uniform causing drag or getting stuck in the tip.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5

    Default

    What is lurchy? Is the roll lurching around, or is it feeding lurchy? Sometimes, the wire will jump on top of the feed roll IF it isn't fully seated in the groove....A lot of it has to do with the tensioning of the spool as well.

    A lot of people are able to get the flux core to feed ok with the regular drive rolls...Some are not. Unfortunately we don't have any in stock in the US and I don't know why. Canada does though. Also, if you are having issues, you may be running the wrong polarity. Are you running negative polarity?

    Why on earth are you running flux core anyway? Overall, its not the best choice.

  6. #6

    Default

    Quote Originally Posted by performance View Post
    What is lurchy? Is the roll lurching around, or is it feeding lurchy? Sometimes, the wire will jump on top of the feed roll IF it isn't fully seated in the groove....A lot of it has to do with the tensioning of the spool as well.

    A lot of people are able to get the flux core to feed ok with the regular drive rolls...Some are not. Unfortunately we don't have any in stock in the US and I don't know why. Canada does though. Also, if you are having issues, you may be running the wrong polarity. Are you running negative polarity?

    Why on earth are you running flux core anyway? Overall, its not the best choice.

    We have it electrode (-) like it should be. It feeds VERY smoothly when we are not welding. We even just squeezed the wire between thumb and forefinger to make sure the feed wasn't pulsing. And it was not pulsing. The roll is seated fine, and not to tight. The arc is what's "lurchy", it's almost like the arc force kicks in and out. Exactly what it is doing: The wire is burning at the end of the puddle, then it burns back up towards the tip, then the amps seem to sweep down allowing the wire to come back to the leading edge of the puddle. This is all happening at 2-4 times per second. As far as why we are using flux core, it's all we have currently, we will be switching to gas as soon as we scrape up some more cash. We played around with the arc force. As my brother was welding I adjusted the Arc Force to about 3 o'clock on the dial. It got really smooth then. The darn thing only came with one 035 tip... I didn't realize this other wise I would have bought a few. Anyway over all we like it very much. Oh, FYI, we had the same pulsy issues on 240VAC as 120VAC. We maintain 119-121VAC while welding so we are good on that. We have our lines boosted to about 124VAC per line because our three phase converter likes a little extra juice. We can run a 15HP 3-phase and a 20HP 3-phase simultaneously. So we have good power. Mark if it better suites you, you can give me a ring. I just talked to you on friday (319)-***-9632
    Last edited by I_Love_Plasma; 01-08-2012 at 02:32 PM.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  7. #7

    Default

    You need to check how tight your nut holding the spool of wire is. It should allow your wire to curl up when you touch the trigger while holding the tip close to a smooth surface. I had my spool way too tight and it constantly sputtered. After I checked the tension on the spool of wire I realized it was to tight.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. IMIG-200 with flux core, running on generator
    By chadford in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 10-08-2011, 10:04 PM
  2. Running PU 205 on 110volt
    By worntorn in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 07-03-2011, 10:12 PM
  3. Still running strong
    By Stelfabulous in forum Customer Testimonials
    Replies: 4
    Last Post: 12-14-2010, 01:11 PM
  4. got it up and running pm256
    By royal in forum Customer Testimonials
    Replies: 1
    Last Post: 07-29-2010, 09:48 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •