Originally Posted by
ozzy
That brings me to my next question. Where do you all purchase material in the Phoenix, AZ area (plate steel/aluminum, bars, etc)? Home Depot has a good selection of steel round/square steel tubing. However, it's probably way over priced....and, I can't get a big flat piece of steel there (say, 3 ft x 5 ft x 3/8") - not sure, since I'm new...

Welcome to the forum.
I would pick up a plate at freeway metals on 19th Av. just north of the I-10 truck route. If you check out my table project I picked up a 5'X4'X3/8" metal table top at Freeway metals for under $200. They have all different sizes in all different thicknesses. They also have good prices for tubing and other things. I typically pick up metal from Industrial Metal Supplies but some times Freeway Metals has better deals and a different selection (better for odd size thick material if needed).