Share
Results 1 to 5 of 5

Thread: Cheap-Skate-Pipe- Rotator

  1. #1

    Default Cheap-Skate-Pipe- Rotator

    Spent twice as much time fooling with trying to hook a door closer and weight to the flat-belt than grinding today.. ended up just looping it under my roller stand and using my toe to turn it. Worked good on the old steam pipe legs. Seems like the big flap disk will probably spin'er by itself. I'm a dope, was using my grinder for most of it.


    Click image for larger version. 

Name:	cs1.jpg 
Views:	500 
Size:	129.5 KB 
ID:	4517Click image for larger version. 

Name:	cs2.jpg 
Views:	521 
Size:	129.8 KB 
ID:	4516Click image for larger version. 

Name:	cs3.jpg 
Views:	541 
Size:	134.0 KB 
ID:	4515
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  2. #2

    Default

    I like it! A cheap, easy way to weld some pipe
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    I was thinking that if I could get the closer hooked up, it would turn it slow and be adjustable. Turns out I've been storing a broken one for 10 years... still in the box.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  4. #4

    Default

    Thats a good idea. I didnt think of using casters to roll pipe like that. Last time I welded pipe, i set it on a slight open vice and welded a little bit between turning it.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  5. #5

    Default

    That is a neat idea, now you'll have to use 2 feet one to roll the pipe and 1 to operate the tig. I haven't had any pipe to weld lately but Ill definitely keep this in mind.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

Similar Threads

  1. looking for cheap leads, any ideas?
    By dennis in forum General Welder Questions
    Replies: 5
    Last Post: 12-13-2011, 12:30 AM
  2. Cheap tubing notcher /holder
    By Jules The Great in forum Hobyist Projects
    Replies: 4
    Last Post: 11-11-2011, 01:36 AM
  3. Plasma cutting 'table' on the cheap- way cheap.
    By qubit in forum Hobyist Projects
    Replies: 5
    Last Post: 10-24-2011, 04:10 PM
  4. Sweet bookcase on the cheap!
    By ScratchStart in forum Personal Projects (no welder required)
    Replies: 2
    Last Post: 05-03-2011, 12:45 PM
  5. Really Cheap $19.98 Tungsten Sharpener
    By JohnS in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 04-21-2011, 04:36 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •