Quote Originally Posted by revkev6 View Post
hey guys, I got a WP 20 size torch from everlast to go with my 225lx. figured it could only make my learning curve easier to have the smaller torch. I have two little issues with the torch and they are both with the consumables kit that it comes with.

The kit comes with two different 2.4mm tungsten Collets. neither one fits right. one is smaller in diameter that I'm guess might go with the short back cap as it is too short/small to work with the long back cap. when I use the bigger collet the back cap only gets about a quarter of a turn before it tightens. Anyone else had fitment problems with the WP20?? what did you buy for consumables to go with it and how did they fit the torch??



my other peave is that the consumables kit comes with only a 2.4mm collet and only #4 size cups. I figured I would get the same array of consumables i got with the 225lx. at the very least that I would get a set of consumables that could be used together. I don't believe there is a scenario out there where a #4 cup is used with a 3/32 tungsten.


My WP20 came with a welder, it only came with a 2mm collet ( not much use in the USA )and 5/16 cup, I had to get other sizes locally. The collet body does screw in tight. The same collets work with the long and short back cap.