Share
Results 1 to 3 of 3

Thread: Plasma cutting with Powerultra 205

  1. Default Plasma cutting with Powerultra 205

    This is the first piece I cut with my new machine. It is 1 of a set of 4 frame tie-in pieces for the rear bumper on my CJ7. It is 1/4" thick, cut very cleanly. What slag remained on the backside brushed off easily with a chipping hammer. There was no grinding done to this piece.

    Question to tech.....I had my machine set at 50 amps 65 psi, is this close to recommended settings for !/4" plate?
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	frame support.jpg 
Views:	538 
Size:	93.8 KB 
ID:	78  

  2. #2

    Default

    Try 30 amps.
    It'll be a little slower, but much more control and a finer cut.

  3. #3

    Default

    Nice looking bracket.
    Wayne

Similar Threads

  1. Cnc plasma cutting problems
    By FeddFab in forum Everlast Plasma Cutters (PAC)
    Replies: 30
    Last Post: 07-28-2013, 11:43 PM
  2. Plasma Cutting Tungsten
    By Scotty1 in forum General Welding Questions
    Replies: 8
    Last Post: 04-07-2012, 09:30 AM
  3. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 12:08 PM
  4. Plasma Cutting
    By Lone Wolf in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 01-09-2012, 02:27 PM
  5. PowerUltra Plasma Issue
    By kenwhite in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 06-10-2011, 09:57 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •