Buggy Chief Argon Flow Rate Conversion on... 01-01-2012, 10:47 PM
Jake98 roughly half the cfh # is... 01-01-2012, 10:59 PM
Buggy Chief Thanks Jake98. I just found... 01-01-2012, 11:03 PM
Jake98 Hey, no problem, I've got at... 01-01-2012, 11:07 PM
Joe from NY I was disappointed myself... 01-02-2012, 12:31 AM
DVA ~3.8 liters per gallon ... 01-02-2012, 01:39 AM
geezer Hi Buggy Chief,,,if you have... 01-02-2012, 11:58 PM
Tritium Excellent information as... 01-03-2012, 04:04 AM
geezer Thanks Turmond,,,always glad... 01-03-2012, 06:19 AM
redbeard Just when I was about ready... 01-03-2012, 07:28 AM
Jake98 Are lenses better than cups... 01-03-2012, 12:30 PM
geezer The advantage I see with a... 01-03-2012, 01:46 PM
Buggy Chief Hey Geezer- Thanks for the... 01-03-2012, 01:48 PM
Jake98 Ditto Geezer 01-03-2012, 01:54 PM
zoama The price of a regular gas... 01-03-2012, 07:13 PM
Previous Post Previous Post   Next Post Next Post
  1. Default Argon Flow Rate Conversion on Tig Calculator

    The Valuable resource that is the Welding Calculator on the Everlast site and Miller Site post the Argon flow rate in denomination of CFH...However the regulator that came with my Everlast PP205 is in LPM.

    Can anyone give any insight into the appropriate conversion? For example aluminum 1/16" with a corner weld calls for 15cfh...what is this in lpm?

    I set my 40 argon tank to 17, however this was in lpm and not cfh and my argon tank ran out in 1 hour

    Thanks for any feedback.

  2. #2

    Default

    roughly half the cfh # is lpm. I did the same thing, almost..
    guys that know what they're doing say to turn it down until you see porosity, then turn it back up a little.
    Last edited by Jake98; 01-01-2012 at 11:05 PM.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  3. Default

    Thanks Jake98. I just found the conversion calculator and you are correct. 15 cfh converts to 7 lpm.

    http://www.convert-me.com/en/convert...olume#ft3/hour

    Thanks again for your response and help.

  4. #4

    Default

    Hey, no problem, I've got at least two hours tig experience now! (one per tank full..)
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  5. #5

    Default

    I was disappointed myself because on the phone with the salesman before I ordered, we discussed the difference between the everlast tig machines and the Miller ones. I mentioned the metric flow meter and I was told that the flowmeters are not calibrated in metric. When i recieved my unit, i found out that was clearly not true. And the funny thing is my manual from everlast mentions a CFH measure, not a metric one.

  6. #6
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    ~3.8 liters per gallon

    7.48 gallons per ft^3

    60 min per hr

    1 [ft^3/hr] = X liters/hr can be calculated as follows


    1 [ft^3/hr] * 7.48 [gallons/ft^3]*3.8 [liters/gallon] = 28.4 [liters/hr]

    Because there are 60 min per hr the 28.4 liters per hour can be divided by 60 to provide a conversion from CFH to liters per minute (LPM).

    28.4 [liters/hr] /(60 [min/hr]) = 0.47 LPM = 1 CFH

    With this number 0.47 being so close to 0.5, just divide the usual CFH by two and this will provide a close conversion for LPM to use for a setting.

    I.E. 15 CFH ~ 7.5 LPM or 20 CFH ~ 10 LPM.

    Hope this helps save some gas.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  7. #7

    Default

    Hi Buggy Chief,,,if you have a regulator marked in litres you are a head of the game,,,cause working in CFH and trying to remember those settings is a PITA, working in litres is so much simpler,,,,first of all you must know your cup size,,,it just so happens that the cup size and the litre settings are nearly the same.

    For example a number 3 cup would be 3 litres, and a 4 would be 4 litres,,,,,this varies somewhat as the amperage increases,,,however as a good rule of thumb you can say,,,,that litres = cup size + 1 up to 200 amps and then litres = cup size + 2 up to 250 amps. (the limit of most single phase tig welders)

    You can check this out by downloading the CK Worldwide tech manual and looking at the chart on the bottom of page 3
    http://www.ckworldwide.com/technical_specs.pdf

    Hope this helps answer your questions.........Knowing your cup size and using the proper electrode size for the amps is the key, setting the gas flow in litres is then easy.
    Some of those lies people tell about me, are true

  8. #8
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Excellent information as usual geezer. Thanks. How does the rule work for gas lens setups?

    Thurmond
    Last edited by Tritium; 01-03-2012 at 04:06 AM.
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  9. #9

    Default

    Quote Originally Posted by Tritium View Post
    Excellent information as usual geezer. Thanks. How does the rule work for gas lens setups?

    Thurmond
    Thanks Turmond,,,always glad to help if I can,,, As far as using a gas lens goes,,,according to the chart on page 3 the rule of thumb would approximate cup size less 1,,,and cup size less 2 in the 200 amp+ range,,,due to the increased efficiency of the lens,,,check out the chart on page 3 and it will give you a rough correlation for that...I find it much easier to remmeber simple rules of thumb and then adjust from there...
    Some of those lies people tell about me, are true

  10. #10
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by geezer View Post
    Hi Buggy Chief,,,if you have a regulator marked in litres you are a head of the game,,,cause working in CFH and trying to remember those settings is a PITA, working in litres is so much simpler,,,,first of all you must know your cup size,,,it just so happens that the cup size and the litre settings are nearly the same.

    For example a number 3 cup would be 3 litres, and a 4 would be 4 litres,,,,,this varies somewhat as the amperage increases,,,however as a good rule of thumb you can say,,,,that litres = cup size + 1 up to 200 amps and then litres = cup size + 2 up to 250 amps. (the limit of most single phase tig welders)

    You can check this out by downloading the CK Worldwide tech manual and looking at the chart on the bottom of page 3
    http://www.ckworldwide.com/technical_specs.pdf

    Hope this helps answer your questions.........Knowing your cup size and using the proper electrode size for the amps is the key, setting the gas flow in litres is then easy.
    Just when I was about ready to get a piece of tape to make an alternate scale, you come along with a much more elegant solution.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  11. #11

    Default

    Are lenses better than cups for some applications or in general?
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  12. #12

    Default

    Quote Originally Posted by Jake98 View Post
    Are lenses better than cups for some applications or in general?
    The advantage I see with a lens over a cup is electrode stick out to reach into tight areas, the lens gives a more directed gas flow, some people try and cheat by using a small cup to get into the tight areas,,, all that does it overheat the cup and the electrode...so yes a lens would seem the way to go but it costs more like everything else that's good. Of course that is stated on page 5 of the CKworld wide tech manual,,,,good reading ,,,see my previous posts to link to it.
    Some of those lies people tell about me, are true

  13. Default

    Hey Geezer-

    Thanks for the helpful tips to a Newbie.

  14. #14

    Default

    Ditto Geezer
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  15. #15

    Default

    The price of a regular gas lens is nothing considering how long they last $9 for a five pack http://www.ebay.com/itm/5-45V43-1-16...item2eb270ea09 and $5 for a ten pack of cups http://www.ebay.com/itm/10-53N59-5-a...item2c5624f9e6

    Tip: if you don't want to buy a bunch of different size gas lenses, just buy one pack of the smallest size you'll use and drill them larger as needed.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. New 250ex: gas flow continues to flow
    By Mcutler in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-17-2018, 01:17 AM
  2. problem with argon flow for new (old) powertig 185 micro (2011)
    By jonnycowboy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 03-31-2014, 01:00 PM
  3. going rate for argon and lease rates
    By dgarnier in forum General Welder Questions
    Replies: 79
    Last Post: 12-29-2013, 04:57 PM
  4. tig argon flow rate ?( l/min and/or scfh)
    By rab in forum General Welder Questions
    Replies: 2
    Last Post: 02-15-2012, 02:20 AM
  5. Argon gauge questions/ball type flow meter
    By Longlasting in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 13
    Last Post: 07-07-2010, 06:00 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •