When I moved to welding aluminum I found that I started melting the edges away. Using the foot pedal I was able to let off a little before the ends keeping them from melting the edge off. I also found that just a couple of amps seemed to make a noticable difference. I think I was using about 46 amps for the same size material as you are welding on.