    Is heating small parts to bend, with a tig torch, an accepted method? I have to make some tie-down hooks, and was thinking that would be an easy way to heat them up.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  2. #2

    Default

    Heating with the tig torch can be done but it is awkward cause you cannot move away without breaking the arc at some point, better to invest in a twin carbon arc torch, once the flame is started you can play across the area being heated and pull away to reduce the heat etc. I have one and it works fine for heating or brazing, a lot cleaner than an O/A set up , but the light is very bright.
    Some of those lies people tell about me, are true

  3. #3

    Default

    What's the material type and size and what shape will you bend it to ?
    Last edited by zoama; 01-01-2012 at 01:48 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Small, something like 1/8 x 1/4 steel bent in a 'u' to hook ratchet straps to. Probably don't even need to heat it..
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  5. #5

    Default

    You shouldn't need to heat it at all for that. If you do want to heat it, you could just use a propane torch to do so.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. replacement parts availability ?
    By 31fords in forum Pre-sales, Sales and Shipping questions
    Replies: 3
    Last Post: 08-30-2019, 04:37 PM
  2. Large Rosebud Heating TIp
    By cbmkr in forum General Welding Questions
    Replies: 2
    Last Post: 08-26-2012, 06:42 PM
  3. I received wrong parts
    By roadymi in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 04-21-2010, 02:33 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •