Share
Results 1 to 5 of 5

Thread: cutting at an angle

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default cutting at an angle

    i have a PP60 with the 80 type torch ? not sure it has a red handle...
    anyways...
    cutting 1/4" mild steel .. the cuts are cutting down at an angle ... the flame is not shooting straight... just started doing this...
    could it be my consumable ? i changed it out lately... hopefully i put it back right...

    running it on about 40 on the setting and 60psi on air...
    no water in the lines , 2 water traps , one on compressor one on plasma

    like mention , havnt had this before... just started doing this....

    thanks
    mat

  2. #2

    Default

    Sounds like you need to change the consumables.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    yeah, i changed the consumables once... did it again ... had the same problem...
    so i turned up the Heat/Amps to 50 , and air down slightly .. and it seemed to have cut alot better.....
    now im confused.... cause i found the right settings when i first got it .. and wrote it down on the machine and kept it same... now i have to add more power to get the samething... hoping my machine isnt going out ....

  4. #4

    Default

    I ordered some consumables with 1.1mm tips http://www.ebay.com/itm/400088136952...84.m1423.l2649 I'll have them tomorrow. They should cut a little cleaner than what came with the P80 torch.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5

    Default

    Quote Originally Posted by McClary View Post
    i have a PP60 with the 80 type torch ? not sure it has a red handle...
    anyways...
    cutting 1/4" mild steel .. the cuts are cutting down at an angle ... the flame is not shooting straight... just started doing this...
    could it be my consumable ? i changed it out lately... hopefully i put it back right...

    running it on about 40 on the setting and 60psi on air...
    no water in the lines , 2 water traps , one on compressor one on plasma

    like mention , havnt had this before... just started doing this....

    thanks
    mat
    Hey Mat, have not heard from you for some time. Happy New Year.

    Quick thing would be swap out the two consumables out and run the amps up to 50. But sounds like you have everything set correctly.

    If that doesn't do it, give us a call 877-755-9353.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Hitachi G12SR3 4.5" angle grinder 6.0 amp
    By jakeru in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 87
    Last Post: 04-25-2014, 12:47 AM
  2. Best Nozzle for Close Angle Merged Exhaust Tubing?
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 01-15-2013, 04:46 PM
  3. Optimal Tungsten Grinding Angle
    By Rivets in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 06-11-2012, 08:49 PM
  4. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 12:08 PM
  5. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •