    Default Lead Cable Size

    Mark what is the cable size on the 140?? 6 or 4 ga. Looks like the originals are around 6 ga maybe. Need to turn the 5' leads into at least 10.

  2. #2

    Default

    Gerry, probably a equivalent would be around a #5 gauge if you can find such a critter.

  3. #3

    Default

    Quote Originally Posted by performance View Post
    Gerry, probably a equivalent would be around a #5 gauge if you can find such a critter.
    I looked at some 6 & 4 ga super flex battery cable at work, and your right what comes with the unit looks to be in between them.
    Maybe I'll get a 10' chunk of 4ga and take the 2 5' sections and splice them together.

  4. #4

    Default

    Insulation will fool you.

  5. #5

    Default

    Quote Originally Posted by performance View Post
    Insulation will fool you.
    Yep, have to look at the core size

Similar Threads

  1. I-MIG 250P Add On Lead Hanger
    By zoama in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 02-16-2014, 04:09 AM
  2. power arc 140 lead up grades
    By tbucketford4 in forum Stick Welding (SMAW)
    Replies: 10
    Last Post: 11-21-2012, 03:15 PM
  3. Replies: 26
    Last Post: 02-22-2012, 12:25 PM
  4. welding cable size.
    By bobwills in forum Stick Welding (SMAW)
    Replies: 11
    Last Post: 09-25-2011, 04:05 PM
  5. collet size vs tungsten size
    By docweathers in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-08-2011, 04:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •