Start amps should be all the way down. End amps as well.
Do not know why you should have a problem with the pedal. Is it working with the 225LX pedal?
Specs are .045".
How low of amps is the HF wavering? Please be specific.
Start amps should be all the way down. End amps as well.
Do not know why you should have a problem with the pedal. Is it working with the 225LX pedal?
Specs are .045".
How low of amps is the HF wavering? Please be specific.
Last edited by performance; 12-22-2011 at 08:09 PM.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Is gap setting a routine maintenance item?
Yes, in any HF start welder.