  1. #2

    Default

    Start amps should be all the way down. End amps as well.
    Do not know why you should have a problem with the pedal. Is it working with the 225LX pedal?
    Specs are .045".
    How low of amps is the HF wavering? Please be specific.
    Last edited by performance; 12-22-2011 at 08:09 PM.