  1. Default Shackle mounts

    Nothing too fancy and sorry for the crappy cell phone picture.

    These are new shackle mounts for my CJ7 I welded up with my powerultra 205. Stck welded with 3/32" 6011 at around 80 amps. I love how this little machine lays down a bead.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	shacklemount.jpg 
Views:	680 
Size:	33.7 KB 
ID:	74  
    Last edited by roadymi; 09-23-2009 at 01:49 AM. Reason: add info

  2. #2

    Default

    They look good. How are you going to finist them, paint, powder coat?
    Wayne

  3. #3

    Default

    If you power coat, make sure you fill the holes. Grinding that out is a pain.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. Default Powder coat?

    It's will be lucky to see Rustoleum. The group that I wheel with try to build capable low budget rigs. We don't place a lot of value on beauty. We build them to use in the woods, quarries, dunes or wherever we can find a challenge. While I can appreciate somebody elses waxed and shined jeep, it's not for me. When I get the chassis done I will prime it and spray a coat of Tractor Supply black on it. The body will likey be painted with a roller. Besides I don't know anywhere that does custom powder coating.

    If anyones interested I will post updated pics as the build progresses. My next project is to build outboard mounting points for the front spring hangers. Progress will slow soon as I drive propane truck for a living and busy season is soon approaching.

  5. #5

    Default

    I bought a gallon from TSC on Sunday. It was on clearance for 19.99. Valspar.
    Black equipment enamel.

Similar Threads

  1. 4bt Cummins motor mounts
    By dzljon in forum Other Custom Fabrications
    Replies: 12
    Last Post: 08-31-2016, 06:14 AM
  2. Anti-roll bar link mounts
    By its_34 in forum On Road Fabrication
    Replies: 5
    Last Post: 08-17-2013, 04:42 AM
  3. Aero bar mounts
    By Rambozo in forum Personal Projects (no welder required)
    Replies: 8
    Last Post: 07-10-2012, 02:28 AM
  4. Project 5 Mean Green Contest, SeanMurphy265, Mobile Home Leaf Spring Mounts
    By SeanMurphy265 in forum Heavy Equipment and Commercial Projects
    Replies: 3
    Last Post: 05-23-2012, 01:26 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •