 Originally Posted by 
todmorg
					
				 
				I've noticed my gas consumption seems high with my new EXT, so I stared looking for leaks.  I found that if I disconnect the hose from the welder and hold my thumb over the end and shut off the tanks, the pressure holds, if I hook it back to the welder and close the tanks, the pressure drops to zero in about 10 seconds.
Are these solenoids repairable or adjustable?
Does it need to be replaced?
			
		 
	 
 Have you used any snoop (soapy water) on the hose fitting to the hose barb see if it is leaking? How tight was the hose on the hose barb and do you have a hose clamp? I had the same thing on my EXT but my hose clamp was not on tight enough.
				
			 
			
		 
			
				
			
			
				Miller 252
PowerTig 250 EXT 
Evolution Rage 2