I just opened my pedal and the black gear on the shaft that turns the pot was slipping. Tightened the set screws and it works great now. the shaft is completely round and the set screw has no leverage. I think this might happen a lot. I'm gonna take it out and grind a land on the shaft, hopefully I won't break anything.