					I bought the Everlast #20 torch and Love it!  A lot easier to use than the one supplied with the 250EX, just less bulky.  AND, everything hooks up, with some other brand torches you will have to find fitting or make something work.
It does sound like a Downslope thing?  Also, you want to hold the torch on the weld when you finish until your post flow stops.
Some guys at welding class would run the bead of weld then back track over the bead about a half inch so they didn't get the "butthole" at the end of the weld.  I have been just dabbing extra filler rod at the ends to fill the hole before it forms.
				
			 
			
		 
			
				
			
			