    When stick welding most or the time its electrode positive but for thin metal you can run it electrode negative and you get less penetration making thin metal easier to weld.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  2. #2

    Default

    Good stuff to know.............Thanx
    PP 205
    Miller Cricket
    Lincoln Stick
    Iwata Airbrushes

Similar Threads

  1. Cnc plasma cutting problems
    By FeddFab in forum Everlast Plasma Cutters (PAC)
    Replies: 30
    Last Post: 07-28-2013, 11:43 PM
  2. Plasma Cutting Tungsten
    By Scotty1 in forum General Welding Questions
    Replies: 8
    Last Post: 04-07-2012, 09:30 AM
  3. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 12:08 PM
  4. Welding/Plasma Cutting Table
    By scootarida1 in forum Hobyist Projects
    Replies: 3
    Last Post: 01-08-2012, 01:44 AM
  5. Plasma cutting with Powerultra 205
    By roadymi in forum Customer Testimonials
    Replies: 2
    Last Post: 09-30-2009, 10:51 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •