    I'm putting a Brass bushing into a steel tube.
    The Brass bushing is flanged so it will butt up to the outer edge of the Steel tubing. There will be a Stainless rod running throught the bushing and I do not want the Brass to rotate in the tube.

    Has any of you ever used a TIG torch to braze Brass to Steel?
    I just read that you use a silcone Bronze filler rod to do it. I have never Brazed anything so I'm wondering how different it is from welding? Is it basically controlled melting?

    I would guess I work the Steel first to get it hot enough to melt then put some heat on the Brass?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    You will need to get a filler rod to join the two of them (well, you may be able to get the brass to flow, but I woudl not recommend it).

    I woudl assume the bushing you are using are actually bronze. Be cautious if they are "oilite" style. If so, they will be a less than 100% dense sintered product that s impregnated with oil or wax. If you heat it, the lubricant will be no more.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    Quote Originally Posted by sportbike View Post
    You will need to get a filler rod to join the two of them (well, you may be able to get the brass to flow, but I woudl not recommend it).

    I woudl assume the bushing you are using are actually bronze. Be cautious if they are "oilite" style. If so, they will be a less than 100% dense sintered product that s impregnated with oil or wax. If you heat it, the lubricant will be no more.
    The filler rod I have seen several people recommend is a "SifBronze #8".
    BUT, I Will be using an oil impregnated Brass bushing so I am changing my plan. I'm going to order a different wall thickness pipe and just press the bushing into the Steel pipe.

    Thanks for clearing that up!!
    I don't have a torch so that is why I was going to use my TIG.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  4. #4

    Default

    I think I would lean towards small torch and silver solder.
    Bill

Similar Threads

  1. Brass And Copper Belt Buckles Project 1
    By cbmkr in forum Metal Art
    Replies: 10
    Last Post: 09-11-2013, 05:50 AM
  2. 12" 200psi Antique Brass Pressure Gauge Repair
    By zoama in forum Personal Projects (no welder required)
    Replies: 12
    Last Post: 02-13-2013, 08:21 PM
  3. Replies: 18
    Last Post: 05-26-2012, 07:00 PM
  4. Frame for stained glass (frame made ​​of brass)
    By donor76 in forum Hobyist Projects
    Replies: 5
    Last Post: 01-06-2012, 12:58 PM
  5. Brazing/Soldering Galvanized Sheetmetal - techniques?
    By jakeru in forum General Welding Questions
    Replies: 20
    Last Post: 10-03-2011, 09:02 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •