i got my new pp256 on monday. so far i have severed 1"plate with the plasma cutter so i was impressed with that. i used the stick, welded some test beads on some 1/4" plate with 1/8" 7018, the welds were beautiful. my problem is in tig mode ac or dc i can't get the arc to start, it just jumps from the tungsten to the metal and never starts.
thanks