    Default Amazing Aluminum Tig Work !!

    I believe this guy sold his soul to the devil in trade for his tig talents !! Ive seen alot of his work and it is awesome to say the least.

    Everlast Powertig 250EX
    Worlds Quickest Oldsmobile Powered Vehicle
    397 cid Twin Turbocharged Oldsmobile

  2. #2

    Default

    Yeah, that is very nice work - I like the fact that starts/stops are well handled. Look at the little injector ports on the intakes at the bottom half, you can see he started at the top and went around and stopped at the top - nice job! Maybe I can do this by 2023....

    Cheers,

    Mike

  3. #3
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by TD2593 View Post
    I believe this guy sold his soul to the devil in trade for his tig talents !!
    Good trade if you ask me, where do I go to sign the contract?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  4. #4

    Default

    I'm gonna say that's all he welds everyday! Probably has some type of jig to keep it in position. Nice looking beads fo-sho!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Looks like Marcella's manifolds.

    I think I've got his style figured out. He uses a Helium/Argon mix; which cuts down on the excessive cleaning action of pure Argon, and makes really nice, shiny looking weld beads. Of course he has developed good torch manipulation skill (applying the right torch angle, etc repeatably on every one of the welds in his manifolds), got his machine settings dialed in, etc.
    http://www.everlastgenerators.com/fo...with-He-Ar-mix
    Click image for larger version. 

Name:	pipe_after_welding_closeup.JPG 
Views:	545 
Size:	42.5 KB 
ID:	4133

    He also sands / "grains" his aluminum stock prior to welding, to give it that "satin brushed" appearance. (In above pictured example, I didn't do that. It just takes some extra time and elbow grease.)

    The consistency of the weld quality throughout his projects is impressive - that takes lots of practice.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  6. #6

    Default

    its beautiful work, i would want to see what thats going on top of, and what its in. that much work into a manifold, i bet the rest of it is also finely crafted
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  7. #7
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    http://www.marcellamanifolds.net/Elbows.html
    http://www.yellowbullet.com/forum/sh...d.php?t=127750

    He has built quite a number. It seems that he primarily does V8 engine applications.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  8. #8
    Join Date
    Jul 2011
    Location
    Southern Middle TN
    Posts
    47

    Default

    Quote Originally Posted by jakeru View Post
    Looks like Marcella's manifolds.

    I think I've got his style figured out. He uses a Helium/Argon mix; which cuts down on the excessive cleaning action of pure Argon, and makes really nice, shiny looking weld beads. Of course he has developed good torch manipulation skill (applying the right torch angle, etc repeatably on every one of the welds in his manifolds), got his machine settings dialed in, etc.
    http://www.everlastgenerators.com/fo...with-He-Ar-mix
    Click image for larger version. 

Name:	pipe_after_welding_closeup.JPG 
Views:	545 
Size:	42.5 KB 
ID:	4133

    He also sands / "grains" his aluminum stock prior to welding, to give it that "satin brushed" appearance. (In above pictured example, I didn't do that. It just takes some extra time and elbow grease.)

    The consistency of the weld quality throughout his projects is impressive - that takes lots of practice.
    Yes it is Marcella's work. Ive always been amazed at his ability, a true art ! He can weld on cast aluminum and make it look better than any Ive seen.
    Everlast Powertig 250EX
    Worlds Quickest Oldsmobile Powered Vehicle
    397 cid Twin Turbocharged Oldsmobile

  9. #9
    Join Date
    Dec 2011
    Location
    Knoxville, Tennessee
    Posts
    93

    Default Argon Helium mix

    I tried running a mixture of Argon and Helium on my 250 EXT this weekend and found it don't like it at all.. The puddle is completely out of control and the heat runs away at an unreal rate... Now later on I had to figure out why this was happening when I've used it for years on every TIG machine I've ever used without issue.. I came to this conclusion after several attempts to correct the issue..

    What I found is the inverter machines operate so much more on DC-EN that the heat gets out of control even backing off the foot pedal.. I discovered that if I set the machine up at 60 HTZ and around 60-40 on the AC balance like a syncrowave type machine that the Helium was well accepted like any other TIG rig... The good news is the Helium at $90 a 330 bottle isn't required on 95% of anything you will do. Why make a modern welder operate like an outdated machine just to use another bottle of gas? I couldn't find a reason to myself...

    If anyone else had experimented with the Helium mixes as well please post up what you discovered as well.. I always enjoy learning new information that will help me and anyone else I may be helping at some time or another be a better welder..

  10. #10
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Gunner - I agree with you that I don't see the sense in running Helium with high % EP... the high EP% just defeats the purpose of using Helium in the first place. I use 20% EP for AC Balance, which is is the minimum that my machine (Super200P) can do. I agree with you, that I would sooner switch away from the expensive Helium and onto pure argon than I would raise the EP%.

    When you tried the Helium mix, did you try a smaller sized tungsten to go along with it? I found a 1/16" tungsten extended the low range (i.e., how thin of metal is weldable with controllable heat) of what the helium mix can do considerably. And I actually am quite impressed by the upper range of what the 1/16" tungsten is capable of, combined with the Helium mix as well. If you haven't tried using a small tungsten with your Helium mix, you should give it a try. (And, don't even be afraid to grind a good taper in the tip! If it needs to, the tip can melt, but you'll be surprised how little it really does melt considering how thick of metal it will weld with the Helium mixed in there!)

    I also find with the small tungsten and the Helium mix, keeping the tip prepared matters less. (Than compared to using pure Argon with the bigger, 3/32" tungsten.) With the smaller tungsten, it's easier to just "burn off" aluminum as needed (if you dip) and just keep on welding, as long as you don't touch the filler to the tip and get a huge blob wicked up onto the tungsten. (No easy fix for that; I try to avoid it.) Any touch up on the grinding wheel also goes super fast with the 1/16".

    Also, what portion of helium you mix in there also makes a big difference. I find I haven't adjusted mine since dialing it in at probably about 2.5 cfh Helium and about 10-12 cfh Argon (that's with a #6'ish gas lens, I think.)

    All that said, I still am somewhat new to experimenting with the Helium mix myself, but those are just my thoughts at the moment on how it can be effectively set up on an inverter.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. procut50 won't work
    By babowtie in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 01-22-2015, 12:37 AM
  2. can't get machine to work on aluminum at home
    By tictac in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 12-16-2012, 04:50 PM
  3. Replies: 8
    Last Post: 11-10-2011, 06:30 AM
  4. Replies: 2
    Last Post: 08-03-2011, 03:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •