    Minimum temperature should be 20° F. Extreme temperatures should be avoided. We prefer for the units be stored above freezing. Capacitors can freeze.
    Last edited by performance; 12-11-2011 at 12:20 AM.

  2. Default

    ok so i should start bringing it in during winter
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  3. #3

    Default

    Quote Originally Posted by performance View Post
    Minimum temperature should be 20° F. Extreme temperatures should be avoided. We prefer for the units be stored above freezing. Capacitors can freeze.
    Wow that high of a "low"....probably should advertise that a little better. I will need to bring mine into the basement. It's already around that here now.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4

    Default

    I went back over some old factory information. 14 degrees F or -10C is absolutely the lowest recommended operating temperature. I say 20 for the safe side of things. I don't think my hands would work in that cold very long anyway. Storage can go a little lower ( and varies on the model) into the single digits but do you want to push it? The whole idea is to take care of your welder as an investment. Just as you wouldn't leave it out in the rain, why leave it to suffer temperature extremes?

Similar Threads

  1. New Everlast Mig welders
    By jchaverri in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 08-05-2014, 08:37 PM
  2. everlast welders
    By ale8one in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 08-07-2012, 11:52 PM
  3. My take on Everlast tig welders
    By srp in forum TIG Welding (GTAW/GTAW-P)
    Replies: 62
    Last Post: 03-03-2012, 03:55 AM
  4. Everlast minimum storage temps.
    By todmorg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 24
    Last Post: 01-29-2012, 08:19 PM
  5. New to Everlast Welders
    By drifterific in forum Introduce Yourself
    Replies: 6
    Last Post: 12-18-2010, 02:18 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •