OK, called Ray.... I'm using 1/16th Tungsten and he recommends smaller Tungsten.
I'll try the torch switch too.

So when I turn the Amperage down all the way and it say "9" while in AC, I should not pay attention to the number and just know that the low mark in AC is 20amps?