Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 29

Thread: CGCINC Project#3: 1000lb. water fountain Many, Many pics

  1. #1

    Default CGCINC Project#3: 1000lb. water fountain Many, Many pics

    My wife and I wanted a water fountain for our patio. We searched the internet and found one we like......

    This one was $1200 plus shipping!!



    So, I made the mistake of saying "I could build that for half that price!"
    Needless to say, my wife jumped all over that, lol..

    So here is my build:

    I used Twelve 80lb. bags of concrete.
    Twelve bottles of Charcoal tint.
    18 bottles of cement fortifier.
    Two sheets of 3/4" plywood for the mold.
    A little chicken wire to reinforce the concrete.
    I also used some other misc. stuff I had laying around as well as Buying some Faux rock wall board.
    I bought a small pond pump to create the flow and I also installed three 20 watt underwater lights.

    It all started by building the forms to pour the concrete into. Once I finished building them, I gave it three coats of gloss urethane to help with releasing from the concrete. After that dried, I sanded with 600 grit sandpaper all the way up to 2000 grit and then coated with a pure Carnuba wax to aid in release.
    Next came mixing and pouring the concrete into the forms.
    Then the tear down and the wait for it to cure. Once it had 60 days of cure time, I painted the inside walls with a concrete epoxy that is water tight and made for concrete ponds. At this time I installed the Faux rock wall and the Fiberglass weir/waterfall towards the top of the rock wall.
    It was made in two pieces...Top and Bottom. It was a huge job moving it from my shop to my house but with a lot of help, we got it in it's place! A little wiring and installing the pump and it was working.
    It is now a permanent fixture at this house and when we sell, it stays!
















    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default









    Fiberglass waterfall test fit....


    This is the only picture I have of it on the patio. I had a total of about $650 in this after it was done
    Last edited by CGCINC; 12-09-2011 at 03:21 AM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    Very nice fountain, at that weight I guess you won't have to worry about theft and leaving itl outside at night, I really like your wood work on the forms, shows me you know what you are doing when it comes to working with wood and making forms, another thing I like is the metal wall finish in your shop, great way to have inside shop walls. all in all a nice and interesting project, thanks for showing it.,
    Some of those lies people tell about me, are true

  4. #4

    Default

    The stone color and the look is great (last picture). It came out really nice.

    What did you move it with? Geezer is right, it's safe outside in the yard, until kids put soap in it.

    Are you gonna wait a little while before you surf the internet with the wife again?? Just kidding, it is very nice.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    Quote Originally Posted by everlastsupport View Post
    The stone color and the look is great (last picture). It came out really nice.

    What did you move it with? Geezer is right, it's safe outside in the yard, until kids put soap in it.

    Are you gonna wait a little while before you surf the internet with the wife again?? Just kidding, it is very nice.
    I used a cherry picker to get it in and out of the truck. The top section wasn't too bad, me and a friend loaded it up, it was heavy but doable.
    That PVC pipe is were all the wires and hoses are ran for the lights and pump. We have two small Koi in it and one Bug eyed Goldfish.

    I have learned to watch what I say around the wife!! I get put to work, lol
    That last pic is ok but it looks better in person.
    Last edited by CGCINC; 12-09-2011 at 05:04 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  6. #6

    Default

    Quote Originally Posted by CGCINC View Post
    I used a cherry picker to get it in and out of the truck. The top section wasn't too bad, me and a friend loaded it up, it was heavy but doable.
    That PVC pipe is were all the wires and hoses are ran for the lights and pump. We have two small Koi in it and one Bug eyed Goldfish.

    I have learned to watch what I say around the wife!! I get put to work, lol
    That last pic is ok but it looks better in person.
    It came out good. Hope it is inside a screen and no raccoons in the area. They like koi and big goldfish. Ours has been emptied a couple times.

    The wife started on me this morning, since I took the day off. fix tile, remove a fan, tear down a section of fence, etc.. I can relate.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    Well, my wife took some photo's of the patio I didn't know about so here is a better look at it finished!







    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  8. #8

    Default

    That is really cool.
    Did you dye the concrete to get the color to match the faux stone?
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  9. #9

    Default

    Quote Originally Posted by Spike View Post
    That is really cool.
    Did you dye the concrete to get the color to match the faux stone?
    Yeah, I used the Charcoal dye and poured a sample and let it dry to make sure of the color.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  10. #10

    Default

    That looks really nice.. I really like the stone touch in the top section. One thing I think I liked about the origional is the way the water is pouring out rather running down the back but thats a minor detail
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  11. #11

    Default

    Quote Originally Posted by Jason View Post
    That looks really nice.. I really like the stone touch in the top section. One thing I think I liked about the origional is the way the water is pouring out rather running down the back but thats a minor detail
    I actually like that better too, But, I originally had it like that and it was too loud, sounded like running water in a bathtub. Now it has a trickle sound. Much better for where its located.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  12. #12

    Default

    That Looks great. Say I was wondering since you have the forms all made up, could you whip one of those up for me real quick. I can pick it up Saturday. Just kidding man, I know that was a-lot of work. Some times it's good to do a project like that every once in a while, it makes you appreciate the work that goes into things we just take for granted.
    Miller Challenger 172 Mig
    Soon to be winner of a Powertig 210 EXT

    Wade Mortenson

  13. #13

    Default

    Quote Originally Posted by Powertig View Post
    Some times it's good to do a project like that every once in a while, it makes you appreciate the work that goes into things we just take for granted.
    For sure! Next time I will just pay the extra money... This was a Huge job!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  14. #14
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by CGCINC View Post
    For sure! Next time I will just pay the extra money... This was a Huge job!
    I'm working my way through all of the threads in the forums so please excuse my comments on an old thread. I am NOT going to show any of these pictures to my wife .... Man, that looks great.

    It looks like you put in a lot of prep work to ensure the release went without a hitch. Two questions, did you ever feel any of that prep work was overkill and how did the actual release go?
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  15. #15

    Default

    Quote Originally Posted by undercut View Post
    I'm working my way through all of the threads in the forums so please excuse my comments on an old thread. I am NOT going to show any of these pictures to my wife .... Man, that looks great.

    It looks like you put in a lot of prep work to ensure the release went without a hitch. Two questions, did you ever feel any of that prep work was overkill and how did the actual release go?
    Not overkill, but Loads of time consuming work! The only problem I had with getting the mold to release was in the basin area, I made the inside walls completely vertical but they really needed a slight angle so it would be wider at the top. I had to basically bust the wood out of it.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  16. #16

    Default

    Quote Originally Posted by CGCINC View Post
    Not overkill, but Loads of time consuming work! The only problem I had with getting the mold to release was in the basin area, I made the inside walls completely vertical but they really needed a slight angle so it would be wider at the top. I had to basically bust the wood out of it.
    I could see that... Around here the way they have the concrete release the forms is they spray them down with oil. It keeps the pores in the wood from absorbing the concrete. It does not seem to affect the finish any. BTW really nice job. I can tell you have put a lot of work in it. Anyone who is going to sand down and radius concrete forms.... Did you save the forms????
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  17. #17

    Default

    have a friend that dose that he use Styrofoam forms he uses gun night sprayer so don't weigh much sorta cool he dose around pool rocks and stuff
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  18. #18

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    have a friend that dose that he use Styrofoam forms he uses gun night sprayer so don't weigh much sorta cool he dose around pool rocks and stuff
    Well that is a lot lighter. Have you seen the house foundations??? The use big blocks of Styrofoam and build walls like Legos. Once the foundation is poured you stack all these forms that interlock with one another. Then you pour the concrete into the form and leave it. The Styrofoam is left behind and it adds insulation to the basement walls.

    If you are into making a project I guess you could carve up the Styrofoam and make shapes.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  19. #19
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Brian Ski View Post
    Well that is a lot lighter. Have you seen the house foundations??? The use big blocks of Styrofoam and build walls like Legos. Once the foundation is poured you stack all these forms that interlock with one another. Then you pour the concrete into the form and leave it. The Styrofoam is left behind and it adds insulation to the basement walls.

    If you are into making a project I guess you could carve up the Styrofoam and make shapes.
    That's pretty cool. Is that a code thing or is it something that was adopted because it was easier / faster / cheaper?

    For custom applications, cutting styrofoam in long clean lines might be a bit tough, no?
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  20. #20
    Join Date
    Feb 2012
    Location
    Indian Shores Beach, FL - U.S.A.
    Posts
    101

    Default

    Looks awesome; now you just need to add some waterproof color changing led lights in the bottom that will shine on the back wall.
    PowerTig 250EXT ordered on 2/20/12 - AluMig~250P - MasterTig~250AC - Matco Mig~Spot Welder - Giaintec CAT250D - Harris Steelworker Oxy/Acet - Henrob DHC 2000 - Van Norman CB1401 - Lagun FTV1 Mill - CM Mill/Drill - CM 13x40 Lathe - CM 7x12 Bandsaw - CM 6x48 Belt Sander - CM 12 Disc Sander - Baldor 3/4HP Buffer - TP 960 Blast Cab - 48~Box & Pan Break - 52~Foot Shear - 20~Ton Press - 80~Gal 7.5HP Compressor - 9' Snap On Tool Box - 30' Stainless Tool Box Workbench - 3M Speedglas 9100Xx

Similar Threads

  1. Project 1.325 CGCINC: Simple Pull-up bar
    By CGCINC in forum Hobyist Projects
    Replies: 13
    Last Post: 06-21-2012, 03:08 AM
  2. CGCINC Project #1 Welding table ... Lots of PICS!
    By CGCINC in forum Hobyist Projects
    Replies: 11
    Last Post: 12-25-2011, 10:36 PM
  3. CGCINC Project#5: Weight Stand
    By CGCINC in forum Hobyist Projects
    Replies: 8
    Last Post: 12-17-2011, 07:45 PM
  4. CGCINC Project#4: Dumbbell weight rack
    By CGCINC in forum Hobyist Projects
    Replies: 11
    Last Post: 12-15-2011, 02:29 AM
  5. CGCINC Project#2: TIG filler rod holders
    By CGCINC in forum Hobyist Projects
    Replies: 9
    Last Post: 12-09-2011, 09:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •