Quote Originally Posted by everlastsupport View Post
You will see you spend most time in the 16-20volt range probably. And 22+ for thicker stuff. No set number but we seem to stay 17-23 for most 1/8" to 3/8" items.

Note, on tack welding, you want to run hotter, 1-2 volts more on thinner material and more for thick.

How that trailer project? You should be able to move along pretty fast one it with a IMIG-200.
Just sitting. I am at work offshore until Jan. 15. Haven't even seen my new MIG and plasma with my own eyes.

Thanks for the info.

On my 200DX I have it dialed in, I guess. It's on DCEN, foot pedal on kill.