Share
Results 1 to 12 of 12

Thread: CGCINC Project #1 Welding table ... Lots of PICS!

  1. #1

    Default CGCINC Project #1 Welding table ... Lots of PICS!

    This is my small welding table.
    It's made out of 2.5" x 2.5" for the lower frame and for the upper frame and angled legs, I used 2" x 2". The top is 33" x 48", 1/2" plate. The 5" locking wheels I bought from NorthernTool for $8.99 each. They support up to 220lbs. each and they work great, the lock on the wheels is much better than the $29ea. wheels I saw at the local Tractor Supply. The adjustable/removeable standing station slides into the front 2.5" tubing and there is a locking bolt on the side to keep it in place.
    It turned out nice and I really like everything about it. The only thing not done yet is a removeable splash sheild for the back. I will be making it removeable so it's not in my way when I roll the table out in the middle of my shop.







    Grounding tab...



    Clamp hanger...



    Adjustable standing station...











    Foot pedal basket...
    Last edited by performance; 12-08-2011 at 03:40 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    A few more pics...









    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    Nice looking table, great everybody shares their projects. We can pick-up some details that we can add to our tables.
    I like your angled standing station.

    have fun
    Tom
    Last edited by acourtjester; 12-08-2011 at 01:53 PM. Reason: spelling

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  4. #4

    Default

    Quote Originally Posted by acourtjester View Post
    Nice looking table, great everybody shares their projects. We can pick-up some details that we can add to our tables.
    I like your angled standing station.

    have fun
    Tom
    Thanks...

    Too bad I screwed up and didn't put "Project #1" for the contest....
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  5. #5

    Default

    I helped you out...edited title. Can't do it everytime for everyone though.

  6. #6

    Default

    Quote Originally Posted by performance View Post
    I helped you out...edited title. Can't do it everytime for everyone though.
    Holy Crap!!!! Thank you sir, I really appreciate it!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  7. #7

    Default

    Wow this is a clean setup. I really like the way you made the table top "float" above. How did u cut the angles in the square tubing that holds the table top?
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  8. #8

    Default

    Quote Originally Posted by scootarida1 View Post
    Wow this is a clean setup. I really like the way you made the table top "float" above. How did u cut the angles in the square tubing that holds the table top?
    I laid out what I wanted on paper.... 2" rise between tubing and 3"s from the edge. Then I cut out the design, transfered it to the 2" tubing and cut it out with a band saw. They didn't turn out perfect like stamped pieces but it worked out ok.

    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  9. #9

    Default

    Nice! I never make anything that nice for myself.

  10. #10

    Default

    Thanks for putting these photos up. I was wondering about the tig pedal on the left does that work for you? I like the simple yet elegant Tig Torch holder and the adjustable Tilting table. that could come in handy for sure..
    Miller Challenger 172 Mig
    Soon to be winner of a Powertig 210 EXT

    Wade Mortenson

  11. #11

    Default foot pedal

    I would guess the foot pedal on the left is just for storage next to the side where the welder is. When I built my foot pedal I put 2 handles on it one for hanging when stored andthe other a moving handle grip.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	finished pedal (2).JPG 
Views:	435 
Size:	118.0 KB 
ID:	4310  

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  12. #12

    Default

    Quote Originally Posted by Powertig View Post
    Thanks for putting these photos up. I was wondering about the tig pedal on the left does that work for you? I like the simple yet elegant Tig Torch holder and the adjustable Tilting table. that could come in handy for sure..
    Thanks for the compliments.....I'm left handed/footed so the pedal to the left is what I like and it's comfortable to put my foot up there even if I'm using the torch switch
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Project#3 from CGCINC. Category: General Welding Repair
    By CGCINC in forum Welding Repairs
    Replies: 5
    Last Post: 12-11-2012, 06:33 PM
  2. Project 1 from CGCINC. Category: Welding Cart
    By CGCINC in forum Other Custom Fabrications
    Replies: 20
    Last Post: 11-30-2012, 09:05 PM
  3. CGCINC Project#3: 1000lb. water fountain Many, Many pics
    By CGCINC in forum Personal Projects (no welder required)
    Replies: 28
    Last Post: 05-09-2012, 04:22 AM
  4. Project 1 from CGCINC. Category: MIG Welding Cart
    By CGCINC in forum Hobyist Projects
    Replies: 28
    Last Post: 04-12-2012, 08:21 PM
  5. bike build (lots of pics)
    By whitehendrix in forum Personal Projects (no welder required)
    Replies: 15
    Last Post: 03-13-2011, 04:57 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •