Quote Originally Posted by NRM View Post
I have never had a problem with the standard 3 series collets but want to try thr wedgw collets. What diffrences have you seen? Pros/Cons?
I have never used lanthanated just pure and ceriated so maybe I will give them a try.
They fit better allowing the gas lens to be fully seated into the head and the backcap will lock your tungsten just as the oring seats. They're made of brass and should last for years of hobby use. Well worth the extra pennies IMO.