Share
Page 1 of 3 123 LastLast
Results 1 to 20 of 58

Thread: Everlast 250 EXT TIG WELDER

  1. #1
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default Everlast 250 EXT TIG WELDER

    Just received the 250 EXT, am I the first one?
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  2. #2

    Default

    Quote Originally Posted by DVA View Post
    Just received the 250 EXT, am I the first one?
    Lets see lots of pictures and videos and stuff... it's hard to come by right now.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Darn it, I wanted to be first.

    How does it look?
    Todd

  4. #4
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    You must be, I haven't even got a shipping/tracking notice yet. This is the first thing I ever bought that had to be shipped by truck.

    Whereabouts are you located?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  5. #5
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    I just fired it up once. This thing is smooth and has a nice clean ark. I need to get a new welding helmet because I have a cheep auto dark helmet that works fin for MIG but did not like the pulsing I played with on the TIG. I am waiting for a gas regulator and could only make it work with a small leak. Could not get the fittings to allow a hose barb on my current regulator.

    Anyway this thing his huge. Check out the size compared to my Millermatic 252.

    By playing with the program it looks like there are 10 programs you can store and adjust when wanted. So if you are stick welding your program will be saved. This is awesome if you have a setting for tacking, welding thin steel, welding thick steel, some AC for aluminum aluminum and so on. This will save time when moving to different welds with out going and reprogramming each feature.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_1944.jpg 
Views:	631 
Size:	133.9 KB 
ID:	4072   Click image for larger version. 

Name:	IMG_1941.jpg 
Views:	629 
Size:	139.6 KB 
ID:	4073   Click image for larger version. 

Name:	IMG_1950.jpg 
Views:	731 
Size:	128.1 KB 
ID:	4074   Click image for larger version. 

Name:	IMG_1946.jpg 
Views:	655 
Size:	136.5 KB 
ID:	4075   Click image for larger version. 

Name:	IMG_1942.jpg 
Views:	669 
Size:	130.4 KB 
ID:	4076  

    Click image for larger version. 

Name:	IMG_1957.jpg 
Views:	750 
Size:	128.4 KB 
ID:	4077   Click image for larger version. 

Name:	IMG_1960.jpg 
Views:	719 
Size:	137.3 KB 
ID:	4078   Click image for larger version. 

Name:	IMG_1945.jpg 
Views:	664 
Size:	137.5 KB 
ID:	4079   Click image for larger version. 

Name:	IMG_1947.jpg 
Views:	683 
Size:	135.3 KB 
ID:	4080  
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  6. #6

    Default

    Nice ! It's a much larger machine than I had imagined. Thanks for the pics.

    Umm... someone's sewn their trousers round ya torch lead.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Yes those that is a genuine dungarees.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  8. Default

    Interesting, thanks for posting.
    Being rated at 250 amps like the plain EX, I wonder why it's so much larger.

  9. #9
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Yes, quite large indeed. Thanks for the preview!

    Any idea what the weight is?

    How is the manual?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  10. #10
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    I opened up the top to see the plug gound (did not get a picture) and the boards fill the entire width of the welder. I suspect it is to make the control boards common among the 250+ amp EXTs. From my memory I thought Everlast had the 315EXT and a 400EXT were going to come out at some time. If that were the case, the room would be needed for the extra boards.

    Anyway it is not that bad in size. I am going to build a cart with and have it sit on a built in water pump. Something like the cart for the Miller Dynasty 350. Can not wait for the gas valve to come in to fire this thing up some more.
    Last edited by DVA; 12-06-2011 at 03:22 AM.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  11. #11

    Default

    Wow that is a whole lot bigger than I thought it would be. How much does it weigh? I have a miller encotig and the 250ext looks bigger than it. This is an inverter tig not a transformer right? I guess thats why EL is bringing out 200ext to compete with Miller dynasty, I guessing it will be smaller. Hope you give a full report when you have it up and running. Good luck with it hope it welds as sweet as it looks.
    Bill

  12. #12

    Default

    315 EXT IS out. Boards are the same roughly.

    BTW, Just completed the manual. Anyone wanting the manual before it gets uploaded to the site, pm me your email

  13. #13
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Quote Originally Posted by redbeard View Post
    Yes, quite large indeed. Thanks for the preview!

    Any idea what the weight is?

    How is the manual?
    Welder shipping said that it was 160 lbs. I would assume the welder is about 100-120 lbs.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  14. #14

    Default

    132 according to factory specs.

    As far as a transformer? lol...go look at a syncrowave or a PT 225lx from lincoln.......then pick one up. They do have wheels though. I've tried to tell people these weren't light weights in any manner.

  15. #15

    Default

    Guys .. manual uploaded !

    link http://www.everlastgenerators.com/manuals.php
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  16. #16

    Default

    Nice job on the manual, it seems to cover all the new features very thoroughly.
    Todd

  17. #17
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    So my welder came with this orange tube about 1/8 inch diameter, anyone know what this is for?
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_1953.jpg 
Views:	519 
Size:	127.5 KB 
ID:	4082  
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  18. #18

    Default

    I just got a call from the delivery truck, mine will be here today.
    Todd

  19. #19

    Default

    Mine just arrived, a few questions-

    1- what are the orange tube, the blue tube, and the 2 prong thing with the chrome ring?

    2- where is the pedal and the flowmeter/regulator?

    3- Is this the proper power cord? It is marked 16amp-250volt.
    the cord itself is marked 2.5mm. that is between 12 and 14 gauge

    4- should the individual strands be exposed on the power cord where it enters the welder?

    5- There is no switch on the back for remote control / panel control, how do you switch?
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	DSC00028.jpg 
Views:	512 
Size:	139.4 KB 
ID:	4093   Click image for larger version. 

Name:	DSC00024.jpg 
Views:	532 
Size:	133.4 KB 
ID:	4094   Click image for larger version. 

Name:	DSC00027.jpg 
Views:	527 
Size:	145.0 KB 
ID:	4095   Click image for larger version. 

Name:	DSC00025.jpg 
Views:	525 
Size:	138.3 KB 
ID:	4096  
    Todd

  20. #20

    Default

    I was going to put on an 8 gauge cord, how do I fasten the ground???
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	DSC00032.jpg 
Views:	507 
Size:	140.3 KB 
ID:	4097  
    Todd

Similar Threads

  1. NEW 2013 Everlast PowerMTS 200 MIG / DC TIG/ STICK WELDER
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 0
    Last Post: 11-22-2012, 02:20 AM
  2. Welded with a Everlast welder
    By srp in forum Customer Testimonials
    Replies: 6
    Last Post: 06-18-2012, 11:40 AM
  3. Replies: 11
    Last Post: 06-24-2011, 04:51 AM
  4. Everlast Tig Welder settings
    By revkev6 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-04-2011, 02:23 PM
  5. Looking to buy my first everlast AC/DC TIG pluse welder!!!
    By briphillipsonebay in forum Introduce Yourself
    Replies: 1
    Last Post: 11-15-2008, 02:15 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •