    I was welding with the 250p today and noticed that the voltage is adjustable from 14.5v to 28.5v is this correct ? The specs say 16v to 26.5v
    Also the Amp display always has a - in front of the number is this normal ?

    I really like this machine, it's very different from my little hobart transformer.
    Last edited by zoama; 12-07-2011 at 04:14 AM. Reason: Had the lowend volts wrong
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. #2
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    With the MIG machine it should be running Constant Voltage, and the current will adjust depending on your stick out and your wire speed. If the I-MIG 250P will hold 28.4 V that is awesome, that is about where my Miller 252 tops out. I have never needed anything past 24 volts on my Miller, with 28.4 Volts that is some serious heat output.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  3. #3

    Default

    Trying recollect a discussion with the factory, and the deviation in that spec I believe...it is because that is the pulse voltage, and the figure they use I believe is based on average voltage.

  4. #4

    Default

    Quote Originally Posted by performance View Post
    Trying recollect a discussion with the factory, and the deviation in that spec I believe...it is because that is the pulse voltage, and the figure they use I believe is based on average voltage.
    I thought I edited my first post earlier, but anyway... it's 14.5 volts at the bottom and 28.5 at the top. I built up the end of a 14ga 2x2 square tube today by welding straight on the edge @ 14.5/100 pulse off. One leg was a hair short on one of the two welding tables that I made out of one old big one.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5

    Default

    Quote Originally Posted by zoama585 View Post
    Another interesting note on the 250p or maybe all inverter based migs is that it won't start an arc if the wire is touching your work when you pull the trigger.
    If you let the wire touch when you pull the trigger, you still get gas and wire feed, but no arc and you'll have to turn the machine off then back on to continue.
    Transformer machines don't do this... not complaining, just noting a difference. I really like my I-MIG 250p.
    that was giving people trouble on the Imig 200. There's a good answer for what causes the machine to not start.

    Can you use the pulse on steel, or is this mainly used for aluminum. One day I'm going to jump up to a 250p or MTS 400. I sold my ebay plasma cutter and I'm gathering up some pennies for an Everlast Plasma. If I get another coupon I may just get a 250p.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  6. #6

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    that was giving people trouble on the Imig 200. There's a good answer for what causes the machine to not start.

    Can you use the pulse on steel, or is this mainly used for aluminum. One day I'm going to jump up to a 250p or MTS 400. I sold my ebay plasma cutter and I'm gathering up some pennies for an Everlast Plasma. If I get another coupon I may just get a 250p.
    You can use the pulse on steel if you'd like or turn it completely off. I didn't like the nozzle being hot (electrified) on the oem torch when welding and the spatter stuck to it like mad. The new 20' profax torch that I bought is perfect on this machine and I highly recomend it.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7

    Default

    I am interested in getting the power i-mig 250p. How do you like it and how is the pulse feature? I never used a mig with pulse before. It seams like this one serious machine. I would give my lincoln up in a second for this machine.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  8. #8

    Default

    Quote Originally Posted by Cippee View Post
    I am interested in getting the power i-mig 250p. How do you like it and how is the pulse feature? I never used a mig with pulse before. It seams like this one serious machine. I would give my lincoln up in a second for this machine.
    That thing is a Cadillac and I absolutely love it. I didn't like the torch that came with it at all so I replaced it with a really nice 20' profax torch. I'm still learning about pulse through experimentation. The manuals (online) are extremely basic and don't offer much in the way of suggestions or examples but I guess people that have taken welding classes don't need that stuff.
    Basic training videos for all the everlast machines (on the virtually empty youtube channel) would be a great asset to everlast.

    I highly recommend the I-Mig 250p.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Tig 250p problem
    By jakesporting in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 09-22-2016, 11:51 AM
  2. i-Mig 250, or i Mig 250p, or i-Mig 400?
    By John71a in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 02-21-2014, 12:16 AM
  3. mig 250p
    By steel in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 17
    Last Post: 01-28-2013, 01:32 AM
  4. 250p ???
    By txshockwave in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 01-05-2013, 01:48 AM
  5. PA140ST operation at 120 volts
    By dblake22 in forum Stick Welding (SMAW)
    Replies: 6
    Last Post: 05-03-2012, 11:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •