I was playing with the low end on some al. pop cans the other night and couldn't weld without burning holes.

The readout shows 24 with the knob turned to the bottom stop. For pop tin thickness it would be nice to go down to around 10-12 amps. My PU 205 goes down this low.

What should the lowest possible amp setting be on the PP256?

I see Jody did some nice welds on pop cans with his EX 256 @ around 10 amps.


thanks