  1. Default argon regulator

    ...haven't been doing much with my welder recently (powerpro 256). when I turned on the argon there was an audible leak.

    at first I thought it was the threads at the gauge so I reapplied the teflon tape. When I tried that it still leaked.

    The whole body of the regulator is cracked. A hairline crack from the gauge to the discharge valve. Scary to think it could have blown off right in my face.

    The unit is around a year and a half old and never seen much use. Never dropped or abused.

  2. #2

    Default

    The warranty is only six months on everything except the welder. My pressure guage failed the second time I opened the valve... Just buy a better quality one and keep welding.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    you are right there. not the kind of regulator I would want to give another try to.

  4. #4
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    '13 Everlast 255EXT
    '07 Everlast Super200P

  5. Default

    thanks for the post and link. I didn't realize that there were that many cases of this issue. I hope none have blown apart and injured anyone.

  6. #6
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Indeed; I feel the same way, and I hope everyone is OK. This is not an isolated occurrence:

    Quote Originally Posted by robsthomson View Post
    The regulator body had a hairline crack running between the gauge and cylinder ports.
    Quote Originally Posted by jakeru View Post
    One of my Everlast flowmeters also had a hairline crack in the main regulator body
    Quote Originally Posted by SimpleSimon View Post
    I just discovered a similar leak on my regulator. A hairline crack from the tank inlet port to the gauge.
    Quote Originally Posted by jas329 View Post
    I heard it leaking quite a bit. ... when I looked down on the body of the regulator I saw a hairline crack.
    Quote Originally Posted by sross View Post
    Tried to set up my new 256 and found the same crack everyone else is talking about
    Quote Originally Posted by djcheetah View Post
    I too have a hairline crack to the gauge and the argon is rushing out through the bypass too.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. Everlast Argon regulator upgrade
    By mcleod in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 06-20-2015, 01:39 AM
  2. Replies: 7
    Last Post: 03-22-2012, 04:46 AM
  3. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM
  4. regulator
    By bobkat in forum Customer Testimonials
    Replies: 1
    Last Post: 03-11-2011, 09:18 PM
  5. Argon regulator leak
    By robsthomson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 29
    Last Post: 01-15-2011, 06:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •