    Default PP256 questions

    Hi everyone, I'm a complete noob and I seem to be having trouble. While trying to stick weld with any rod I start in the middle of the recommended amperage range and see how it goes. I always end up passed the recommended amperage or higher to get a "reasonable" bead and get the frying bacon sound. Its tough to know the right amperage when your just starting but the beads look better past the upper recommended amperage. So... is this normal or is my PP256 not "calibrated" correctly?

    I had my wife watch the display that was set at 120 amps and I ran a bead and she said it only dropped to 117 amps while welding.

    I've had to do this with 3/32 6013, 6011 and 1/8 6011 all DCEP
    PP256 with Trafimet A81 plasma torch
    Everlast welding cart

  2. #2

    Default

    Not to worry about being higher than the mid range, there are a multitude of reasons for that, voltage to the welder, length of lead, poor grounding clamp and the mill scale,brand and condition of rods etc and the list goes on, Thing is, your readout may or may not be accurate etc. Point is, such a readout and the midrange are a starting point for you to use as a reference for your machine, that's all. Two identical machines operating from the same plug can vary with each other. Your machine has it's own personality, get to know it and don't fret about it.

    Personally I think your readout is correct and is showing the effect of the varibiles, so not to worry about the readout being calibrated etc.
    Last edited by geezer; 11-19-2011 at 01:19 AM.
    Some of those lies people tell about me, are true

Similar Threads

  1. Newbe with PP256 Some questions.
    By Lakerol in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 10-26-2015, 04:03 PM
  2. pp256 need help
    By Tallguy64 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 0
    Last Post: 04-23-2015, 05:15 AM
  3. Pp256
    By scorp765 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 05-19-2011, 01:20 AM
  4. TG AC pp256 need help.
    By Racecar in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 03-15-2011, 06:11 AM
  5. PP256 set up
    By ryanfull in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 03-11-2011, 06:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •