Hey everyone, so I've had my 225LX for a little while now and I'm really happy with the way it welds. The only problem I've been having is actually starting an arc. On every other machine i've used (miller 350, lincoln 185) I've been able to strike an arc just by holding the TIG torch slightly above the workpiece and depressing the foot pedal. On this machine however, I can't seem to do that. I have to physically touch the tungsten to the workpiece in order to get anything. Is this just the way these welders are or is there something I can do about this? Has anyone else had this problem?