Originally Posted by
67cudafb
I am getting itch to drag out my gs1100e suzuki been sitting in garage for about 15 years. A friend tells me I need to clean gas tank and line it with red kote, anybody have info on the good bad and ugly?
If the tanks is rusty, The coating available at the link below, Caswell Plating, is much better than the "old school" methods.
John
http://www.caswellplating.com/aids/epoxygas.htm
Everlast 200DX
Everlast PT185
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile