Thread: spool gun questions

  1. #1

    Default spool gun questions

    I searched the forum with no success so Here goes

    What contact tip and other consumables do I use for the SM-200-N spool gun?

    The spool gun did not come with any nomenclature so Being a novice I have no idea other then what the Miller welding calculator lists and what little I could find on the web. I will be welding Aluminum, or at least trying to.
    so any heads up on base settings would be great.
    My welder is the I mig 205 and supports a spool gun so I am just looking for the settings to get me started for welding aluminum with .035 wire and argon gas
    Does aluminum mig need to be done with spray transfer mode?
    Thanks
    Ray
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  2. #2

    Default

    The tips are the same as the mig gun (TWECO 11 series.) I believe the others cons are as the same as the mig gun as well, though these are either going to be equivalent to Binzel or Trafimet. You need to buy one size larger tip so the aluminum won't swell and seize in the tip due to the heat and expansion of the aluminum..

    All aluminum should be welded in spray transfer. Its not hard to do, but you'll need to play with it until you get a nice, clean hiss. Keep plenty of contact tips handy while you are learning.

  3. #3

    Default

    Hello
    The SM 200-N spool gun use parts compatable with Binzel 24KD type mig gun and the contact tips are metric M 6 thread ,tweco 11 style tips will thread in my SM 200-N spool gun...
    Regards
    Bob
    Last edited by Doxie; 10-25-2011 at 07:01 PM.
    Trermal Arc T-Bird 270 Amp gas welder gen
    Thermal Arc Pro Wave 185
    PowerArc 200
    power Imig 205
    SM 200-N mig spool gun
    Riland 60 Plasma
    HF 40 Plasma
    ReadyWelder II
    180 Amp Diesel Welder Gen
    Henrob Torch
    Arcair K4000
    2 Ox-Aect outfits

Similar Threads

  1. Spool Gun with i-Mig 205
    By cheebster in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 10-03-2015, 07:44 PM
  2. Spool gun
    By Yofish in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 8
    Last Post: 03-16-2014, 11:55 PM
  3. Why can't I add a spool gun to my TIG?
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 11
    Last Post: 07-21-2011, 10:12 PM
  4. SM 200-N Spool Gun ???
    By kenwhite in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 05-23-2011, 01:08 AM
  5. Spool Spool / Roll Adaptor for Power IMIg250P, DYI
    By Ray in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 08-10-2010, 08:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •