    CK Worldwide and weldcraft specify a minimum of 1 quart per minute of coolant flow to achieve the published power and duty cycle ratings for their TIG torches.

    I've had a watercooled TIG torch lead failure happen before, from using an underpowered cooler pump. The coolant simply boiled away and the power cable overheated near the machine:
    Click image for larger version. 

Name:	IMG_0008.jpg 
Views:	444 
Size:	146.2 KB 
ID:	4139

    That happened using this pump that just sat in the bottom of a bucket. (I think it was called an "aquarium pump"; reminds me of what you posted above.) After the failure, I measured the flow and through those leads (they were 25' long), and I found the flow with that bucket pump was barely mustering .25 quart per minute. Less than 1/4 of what the manufacturer specified:
    Click image for larger version. 

Name:	IMG_0005.jpg 
Views:	424 
Size:	143.0 KB 
ID:	4138

    After switching it to city water pressure, the flow increased to a little over 1 quart per minute, and this extra flow was able to keep the new torch leads cool.

    If you had shorter 12' long TIG torch leads, (rather than the longer 25' versions,) that would help increase the flow and cooling as well. I would advise at least measuring the flow, so you know what you've actually got.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  2. Default

    Did they spec the maximum inlet temperature at 1 quart/min?
    That would allow one to measure radiator effectiveness.

  3. #23
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I have not seen that specification listed anywhere before. It might be worth a call to CK Worldwide, though, they do pick up their phone. If you get an answer, let us know what it is.
    http://www.ckworldwide.com/technical_specs.pdf
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. Default

    I stuck one together a few years ago for the nice little Flex Lok 230 amp torch I'd gotten used to using in the local CC welding classes. It's got those great superflex hoses/cables, makes the one that came with my 200 DX seem like wrestling with a firehose by comparison (but I do like that handle switch). They're only 12.5 feet long but I couldn't move enough water by using some of the cheap pumps I tried. I found a nice one of those carbonator pumps on Craigslist for $30 (just motor/pump, no tank). Big and heavy but nicely built to the point that it looks like it will run forever in my garage. It looks like the typical asking prices have crept up a bit so it may take a bit of patience or luck to come across a great deal.

    Gary

  5. #25

    Default

    I have looked at the flojet's - but they are a bit expensive. If you drop $150 on the pump, and then buy other materials, and labor, it might make more sense to drop $450 on a Everlast cooler with a warranty.... :-) (just joking).

    Which particular pump did you select?

    Cheers,

    Mike

  6. #26

    Default

    If you are not going with an Everlast cooler. The Procon pumps are nice. Brass, expensive, but nice. Pump alone is about 35% of the retail of our cooler.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Everlast 250EX and water cooler question...
    By Lucky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-04-2015, 01:06 AM
  2. Tig cooler cooler power source - "warning"
    By Odyknuck in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2012, 10:37 PM
  3. powerpro 256 water cooler question
    By bubbas55 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 10-28-2012, 07:28 PM
  4. Tig Cooler - PowerCool W300 Question
    By johnnyfive in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 05-03-2012, 11:29 AM
  5. Question about W300 water cooler???
    By DisWeld in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 08-03-2010, 11:28 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •