Does any one know where I can get an affordable upgrade,That will work with my Powerultra 205? Everything else seems to work fine except for the pedal. I had a self enflicked problem that Mike helped to troubleshoot. I was given the wrong gas to tig weld. Gas has to be pure Argon to tig weld mild steel. Thanks Mike! so far the powerultra 205 is a great little combo welder. Someone just needs to rethink the foot pedal. Pedal angle is to steep, spring tension is a bit much.