250 EX 5th breakdown
		
		
				
					
					
				
				
		
			
				
					Thought i would jump on here to try and encourage a response from Everlast about our 5th time broken down 250ex. It is not a year old and has an issue every time we need it. I have performed repairs as guided by tech support but the problems come back, telling me the bad chips are a symptom not the problem.
   I am pretty sure we just got a rare green lemon and would appreciate any info to help expedite the process of having it replaced under warranty. I can not continue to spend our time and money repairing what seems to be a bad machine.
				
			 
			
		 
			
				
			
				
			
			
				Lincoln Power Mig 255
Lincoln Pro Cut 25
Power Tig 250ex and 300 cooler